PYRAN® Platinum Fire-Rated Glass-Ceramics

Product Variants of PYRAN® Platinum Fire-Rated Glass-Ceramics

PYRAN® Platinum is available as three different products: the monolithic glass-ceramic PYRAN® Platinum, the laminated PYRAN® Platinum L, and PYRAN® Platinum F, which features a surface-applied film. PYRAN® Platinum L and F offer high impact resistance alongside protection from fire, hot gases and smoke.
PYRAN® Platinum

PYRAN® Platinum

PYRAN® Platinum fire-rated glazing material is made from the world’s first and only floated transparent glass-ceramic. It is intended for use in non-impact, non-safety-rated locations such as transoms and windows with fire-rating requirements up to 90 minutes.
PYRAN® Platinum

CHARACTERISTICS

With a thickness of 3/16" (5 mm), PYRAN® Platinum provides fire protection for up to 90 minutes with the required hose-stream test. Clear and colorless, the glass-ceramic also offers a smooth surface and distortion-free mirror finish, making it ideal for architectural applications.


YOUR ADVANTAGES

  • Available in sheet size 51 x 99” – the largest in the industry.
  • Weight: 2.6 lbs/ft²
  • Can be used to construct insulated glazing units.
  • Able to be lightly sandblasted or delivered with surface-applied opacity film without affecting the fire-rating.
  • Produced without the hazardous heavy metals antimony and arsenic.
PYRAN® Platinum L

PYRAN® Platinum L

Thanks to an added lamination process, this impact- and fire-rated glass-ceramic is designed to be used in doors and windows with a high risk of accidents. PYRAN® Platinum L not only remains intact after heavy impact, but features the same high resistance to heat and thermal shock as PYRAN® Platinum.
PYRAN® Platinum L

CHARACTERISTICS

With a thickness of 3/8” (9 mm), PYRAN® Platinum L provides fire protection for up to 90 minutes in windows and up to three hours in doors, both with the required hose stream test. Clear and colorless, the glass-ceramic also offers a smooth surface and distortion-free mirror finish, making it ideal for architectural applications.


YOUR ADVANTAGES

  • Available in sheet size 51 x 99” – the largest in the industry.
  • Transparent and wireless.
  • Weight: 4.3 lbs/ft².
  • Achieves the positive pressure test standard UL 10C.
  • Can be used to construct insulated glazing units.
  • Can be lightly sandblasted or delivered with surface-applied opacity film, without affecting the fire-rating.
  • Produced without the hazardous heavy metals antimony and arsenic.
  • Impact rating: ANSI Z97.1 (Class A) and CPSC 16CFR1201 (Cat. I and II).
PYRAN® Platinum F

PYRAN® Platinum F

Ideal for safety-rated locations such as windows, door lites, transoms and sidelites, PYRAN® Platinum F features a surface-applied safety film that adds impact resistance to outstanding heat resistance. With the same thickness, sheet size, fire rating and stunning appearance as PYRAN® Platinum, this variant adds an extra layer of safety to your doors and windows.
PYRAN® Platinum F

CHARACTERISTICS

Designed to withstand impact as well as heat, hose stream and thermal shock, this clear, colorless glass-ceramic is fire-rated for up to 90 minutes in windows and up to 180 minutes in doors. Achieving the positive pressure test standard UL 10C, PYRAN® Platinum F can also be lightly sandblasted or delivered with surface-applied opacity film, without affecting its fire rating.


YOUR ADVANTAGES

  • Available in sheet size 51 x 99” – the largest in the industry – and a thickness of 3/16” (5 mm).
  • Weight: 2.6 lbs/ft².
  • Microfloat production process results in a smooth surface and distortion-free mirror finish with surface-applied safety film.
  • Clear and colorless without a distracting amber tint.
  • Can be used to construct insulated glazing units.
  • Produced without the hazardous heavy metals antimony and arsenic.
  • Impact rating: ANSI Z97.1 and CPSC 16CFR1201 (Cat. I and II).

Want to know more? Let's talk

Whether you need more information, samples, a quote, or advice for a project, I would be delighted to talk to you.

Contact us
Daniel_Poling_1-46.jpg

Daniel Poling

Business Development & Sales Manager