Product Variants of Pharmaceutical Type I Glass Tubing
With their low alkali content, chemical resistance, and optional UV protection, the various forms of FIOLAX® and BORO-8330™ glass provide a very low risk of drug-container interaction. Along with DENSOCAN® and DENSOPACK® transit protection, we offer all-round packaging solutions for the medical professional.
FIOLAX® Pro – The glass of the future
Superseding FIOLAX® clear, it marks the beginning of a future-ready transition for the industry – because patient safety starts with us.
PROPERTIES
FIOLAX® Pro borosilicate glass delivers on the fundamental industry requirements: safety, efficiency, and PCF reduction.
The glass prioritizes safety with superior extractables & leachable profile leading to minimal drug container interaction. It has a high hydrolytic resistance due to constant glass composition. Absence of any heavy metals leads to easy compliance with ICH Q3D as improved Type I glass type compliant with all international regulations: Ph.Eur., USP, JP, ChP, YBB, REACH, RoHS. Efficiency is ensured through smooth machinability during converting and fill-and-finish processes. High output by first-class cosmetic quality, high precision by dimensional accuracy, customizable zero-defect options supported by digital quality documentation via perfeXion® makes the glass highly efficient.
PCF reduction is embedded with the optional FIOLAX® Pro OCF product line, which is expected to be available beginning in 2027 with an approx. 50% lower product carbon footprint*. This is enabled by an electric melting tank, powered by 100% of electricity in the melting process covered by renewable energy Guarantees of Origin. Only in the separate refining unit and in the working tank natural gas is still used.
*Calculation of greenhouse gas emissions from cradle-to-gate per kilogram of saleable glass tubing compared to the market average for borosilicate glass tubing [average value according to ecoinvent 3.10; glass tube production, borosilicate // DE]. The value currently calculated is based on empirical values and simulation data. Relevant information about the FIOLAX® Pro OCF product line and the electrical tank can be found in the implementation plan
YOUR ADVANTAGES
-
Superior chemical quality due to an improved extractables & leachables profile.
-
Optimal processing into the container and subsequent storage of the medication due to constant glass composition
-
Contains no heavy metals like arsenic, antimony or tin in its glass composition
-
Ensured by our proven 100% perfeXion® production, the excellent material quality and tight tolerances enable smooth machine operation during container production and drug filling
-
Refined cosmetic quality achieved through reduced airline presence, including critical inside open airlines, eliminating possible effects on syringe/ cartridge sterility
-
Availability of actual quality data – for each pallet of tubes, generated from 100% individual tube testing
-
Adaptable specifications (best value options) are available to achieve even tighter tolerances or lower defect rates for the most demanding applications.
-
Customizing options such as different tube ends and an anti-scratch coating for safe transport are available.
-
Compliance with all international regulations, including Ph.Eur., USP, JP, ChP, YBB, REACH, RoHS
-
Tighter tubing tolerances than ISO standards for syringes and cartridges
-
Enabling a valid PCF calculation of your products through detailed PCF data based on a transparent calculation method
FIOLAX® clear
CHARACTERISTICS
This high-quality Type I borosilicate glass boasts an outstanding chemical and hydrolytic resistance, impermeability, and neutrality. These properties protect the contents from premature aging and loss of effectiveness. FIOLAX® clear is a secure packaging medium for injectable solutions and biotech products.
YOUR ADVANTAGES
-
Proven since 1911 and registered with thousands of drugs, FIOLAX® clear demonstrates an impressive track record.
-
100% perfeXion® production combines high quality and tight tolerances that contribute to stable machine operation in converting as well as fill and finish. Actual quality data from this 100% single tube inspection are provided for each pallet.
-
Customizable specifications (Best value options) available to achieve tighter tolerances or lower defect rates for the most demanding applications.
-
Customizing options available such as different Tube-End Finishes and Anti-Scratch Coating for safer transportation. In addition, we offer FIOLAX® clear with Controlled Hydrolytic Resistance (CHR), ensuring certified chemical quality of the tubing's inner surface. In case you focus on enhanced mechanical durability, FIOLAX® clear with Optimized Strength (OS) might be the appropriate solution.
-
Compliance with all international regulations, including Ph.Eur., USP, ISO, JP, ChP, YBB, REACH, RoHS.
FIOLAX® amber
CHARACTERISTICS
FIOLAX® amber is a colored glass with a proven track record for securing the long-term stability of light-sensitive drugs. The stable composition of this Type I glass ensures a consistent amber color and therefore light protection, which is created by the addition of iron and titanium oxide. As with FIOLAX® Pro and clear, FIOLAX® amber possesses outstanding material quality with narrow tolerances, resulting in smooth machine operation and superior product quality.
YOUR ADVANTAGES
-
Protection against ultraviolet light for a safe storing of light sensitive drugs.
-
100% perfeXion® production combines high quality and tight tolerances that contribute to stable machine operation in converting as well as fill and finish. Actual quality data from this 100% single tube inspection are provided for each pallet.
-
Customizable specifications (Best value options) available to achieve tighter tolerances or lower defect rates for the most demanding applications.
-
Customizing options available such as different Tube-End Finishes and Anti-Scratch Coating for safer transportation.
-
Compliance with all Type I regulations, including Ph.Eur., USP, ISO, JP, ChP, YBB, REACH, RoHS as well as light protection requirements for parenteral drugs according to Ph.Eur. and USP based on ISO dimensions.
BORO-8330™
CHARACTERISTICS
Like FIOLAX® Pro, clear and amber, BORO-8330™ glass has a consistent composition. In contrast to the other Type I glasses, it is free of alkaline earth metals and has minimum aluminum content. As a Type I Class A glass, it is fully compliant with international regulatory standards, and especially popular for vials and ampoules in the United States.
YOUR ADVANTAGES
-
100% perfeXion® production of BORO-8330™ glass tubing for vials OD ≥ 15mm combines high quality and tight tolerances that contribute to stable machine operation in converting as well as fill and finish. Actual quality data from this 100% single tube inspection are provided for each pallet.
-
Customizing options available such as different Tube-End Finishes and Anti-Scratch Coating for safer transportation.
-
Compliance with all international regulations, including Ph.Eur., USP, ISO, JP, ChP, YBB, REACH, RoHS.