Product Variants of Glass Tubing with High UV Transmission

Thanks to their high transmission in the UV range, there is considerable potential for SCHOTT 8337B, RayVolution D 99 and 8347 glass tubing to be engineered into products that serve a wide variety of applications in lighting and light sensoring.
SCHOTT 8337B

SCHOTT 8337B

SCHOTT 8337B borosilicate glass tubing provides high UV transmission.
SCHOTT 8337B

CHARACTERISTICS

This makes it especially suitable for the manufacture of UV lamps and detectors, as well as photomultipliers.


YOUR ADVANTAGES

  • Offers the possibility for direct sealing to the alloy Kovar or tungsten.
SCHOTT 8347

SCHOTT 8347

This borosilicate glass tubing features high UV transmission as well high hydrolytic resistance.
SCHOTT 8347

CHARACTERISTICS

Due to its high hydrolytic resistance it can be used for water disinfection purposes as well as light guides.


YOUR ADVANTAGES

  • High UVC transmission.
  • Higher IR transmittance (Infrared) than standard borosilicate glass tubing 3.3.
SCHOTT RayVolution® D 99

SCHOTT RayVolution D 99

This so called "soft glass" similar to sodalime glasses – is highly UV transmitting.
SCHOTT RayVolution D 99

CHARACTERISTICS

This makes it especially suitable as envelope for germicidal lamps (low-pressure mercury vapour discharge lamps).


YOUR ADVANTAGES

  • Outstanding high UV-C transmissivity.
  • High geometrical and cosmetic quality.
RayVolution® L 41 for UV LED

RayVolution® L 41 for UV LED

SCHOTT RayVolution® L 41 wafer own excellent UVC transmission values and also convinces with its sealing behavior.
RayVolution® L 41 for UV LED

CHARACTERISTICS

Besides its excellent UVC transmission values, its thermal expansion is very close to aluminium nitride.


YOUR ADVANTAGES

  • Glass wafer for LED optics.
  • Facilitates the optics manufacturing for LED Package on wafer level.
Discs for UV sensors

Discs for UV sensors

Discs for UV sensors SCHOTT 8337B round or square discs are designed for use in photomultipliers and other sensors.
Discs for UV sensors

CHARACTERISTICS

These discs offer outstanding UV transmission and low solarization.


YOUR ADVANTAGES

  • Form is ready for installation without further processing.
  • Direct sealing options with common electrode materials.

Want to know more? Let's talk!

Whether you need more information, samples, a quote, or advice for a project, I would be delighted to talk to you

Man in glasses in business office on phone while working on laptop

1 Step 1
2
3

* Required field

SCHOTT will only use your data to respond to your inquiry. For more information, please click here.