Technical Details of CompRite™ Compressor Terminals

Compressor terminals serve as feedthroughs for the wiring that supplies power to compressors. CompRite™ compressor terminals are manufactured using compression glass-to-metal sealing, delivering hermetic electrical insulation with high mechanical strength. CompRite™ compressor terminals provide high performance and excellent durability over long periods, even in harsh operating conditions such as extreme temperature, pressure, humidity, and vibration.

Features of SCHOTT compressor terminals

High pressure resistance

CompRite™ compressor terminals provide excellent pressure resistance across a range of compressor applications, including ones using CO₂ (R744) refrigerants, where high pressure resistance is especially important.

Excellent electrical insulation

SCHOTT's compressor terminals with optimized electrical insulation combine glass, rubber, and/or ceramic insulating materials with stringent, well-established manufacturing processes.

Vacuum-tight hermeticity

Prevention of refrigerant leakage is crucial to sustain proper compressor functionality. CompRite™ compressor terminals deliver vacuum-tight hermeticity with proven hermetic compression glass-to-metal sealing technology.

Highly resistant to adverse conditions

Compressors operate in demanding conditions, including extreme temperatures, humidity, pressure, and vibration as well as harsh chemicals. The reliable performance of CompRite™ compressor terminals keeps compressors functioning, even in harsh conditions.

Automotive AC e-Compressor Terminals

 

SCHOTT E-Compressor Terminals_composing

Materials

Pin:   Fe-Cr, Cr-Cu, Cu cored Fe-Cr
Eyelet:  Fe
Glass:  Soda barium glass
Insulation material:  Glass, Rubber, Ceramic

Characteristics

Air tightness:  ~ 1.0 × 10⁻9 Pa m³/sec 
Insulation resistance:  1000 MΩ min. at DC500 V
Pressure resistance (air):  4.0 MPa min
Control of base surface roughness:  Ra 1.6~3.2, Rz12.5~

 

Voltage Electric Current Pin Material Pin Diameter (mm) Insulation Material (Rubber) Insulation Material (Ceramic)
24 V - 48 V 80 A - 150 A Cr-Cu 4.0 - 6.0 Optional Optional
200 V - 500 V Up to 30 A Fe-Cr 3.2 Optional Optional
200 V - 500 V   30 A - 50 A  Cu cored Fe-Cr  3.2  Optional Optional 
800 V  Up to 30 A  Fe-Cr  3.2 Yes Yes 
800 V   30 A - 50 A  Cu cored Fe-Cr   3.2 Yes  Yes 

 

Compressor Terminals for Refrigeration & Air Conditioning

Compressor terminals for Refrigeration & Air Conditioning

CO2 Compressor Terminals

CO2 Compressor Terminals

Want to know more? Let’s talk

Whether you need more information, samples, a quote, or advice for a project, we would be delighted to talk to you.

Contact us
Kurtis Kanne Portrait

Kurtis Kanne

Director of Sales