22.09.2014, Landshut, Mainz
SCHOTT expands its range of highly resistant sealing glasses for use in fuel cells
The broad range of high-performance sealants now also includes strontium- and barium-free glass solders for low- and medium-temperature SOFCs
Landshut, Germany, September 22, 2014 – The international technology group SCHOTT offers a broad range of sealing glasses for use in solid oxide fuel cells (SOFCs). These glass solders help to hermetically seal cells and stacks that consist of metallic and ceramic compounds. They are used with nearly all types of fuel cells and provide significant advantages, especially for high-temperature SOFCs, due to their high resistance to heat. Strontium- and barium-free sealing glasses have now been added to the product line. These can be applied to metal alloys that contain a share of chromium and are thus also suited for use in low- and medium-temperature fuel cells. Sealing glass stands up to the harsh environmental conditions and high operating temperatures inside fuel cells and thus contributes to their durability. SCHOTT has been developing glass and glass-ceramic sealing glasses for use in fuel cell technology for 25 years and ranks as a world-leading manufacturer of glass solders. The company will be presenting its materials at the Asian SOFC Symposium in Busan, South Korea, from September 21 to 24, 2014.
Landshut, Germany, September 22, 2014 – The international technology group SCHOTT offers a broad range of sealing glasses for use in solid oxide fuel cells (SOFCs). These glass solders help to hermetically seal cells and stacks that consist of metallic and ceramic compounds. They are used with nearly all types of fuel cells and provide significant advantages, especially for high-temperature SOFCs, due to their high resistance to heat. Strontium- and barium-free sealing glasses have now been added to the product line. These can be applied to metal alloys that contain a share of chromium and are thus also suited for use in low- and medium-temperature fuel cells. Sealing glass stands up to the harsh environmental conditions and high operating temperatures inside fuel cells and thus contributes to their durability. SCHOTT has been developing glass and glass-ceramic sealing glasses for use in fuel cell technology for 25 years and ranks as a world-leading manufacturer of glass solders. The company will be presenting its materials at the Asian SOFC Symposium in Busan, South Korea, from September 21 to 24, 2014.

Sealing glass paste from SCHOTT allows for the components in fuel cells to be hermetically sealed. Source: SCHOTT
SCHOTT’s sealing glass hermetically seals and joins the individual stacks or cells without any tension in both planar and tubular fuel cells. High temperatures and humidity put a significant strain on the materials the cells are made of. Compared to other sealing options, using sealing glasses as an insulation material provides an advantage in that the glasses remain sealed gas-tight over the long term, even when exposed to high temperatures and thermal cycles. Special glass also offers good electrical insulation properties and is chemically stable even under reducing and oxidizing conditions. To achieve high efficiency of the fuel cell and the longest possible lifespan, the glass solder must be made to match as closely as possible the thermal expansion coefficients of the metals and ceramics to be joined in the stack of the fuel cell.
SCHOTT has unique know-how, particularly when it comes to joining glass with metal and ceramics for reliable and durable seals. The company has ranked among the world’s leading manufacturers of specialty glass for 130 years, and its Electronic Packaging division has more than 70 years of experience in manufacturing hermetically sealed housings. The development and production of application-specific sealing and soldering glasses represents the key to achieving a long-term seal.
For further information, visit https://www.schott.com/epackaging/english/glass/powder/fuel_cells.html
Background information:
A fuel cell offers a way of generating electricity and heat in a decentralized manner. Electrical energy is generated in a direct and highly efficient way by leveraging the chemical reaction between hydrogen and oxygen. Due to its high operating temperatures, between 600°C and 1,000°C, a high temperature fuel cell is also capable of using fossil fuels directly as a provider of hydrogen. The existing infrastructure for natural gas, biogas, heating oil, and diesel fuel can thus still be used in a flexible manner. The waste heat from the high temperature fuel cell is then used to generate heat. More than 10,000 heating fuel cells are currently being used in Japan and approximately 600 in German homes. The market is young and continues to grow. Research activities are expanding in Japan, the United States, South Korea, and Europe.
Download link: http://www.schott-pictures.net/presskit/258062.sofc
More press photographs can be found here: www.schott-pictures.net
SCHOTT is an international technology group with 130 years of experience in the areas of specialty glasses and materials and advanced technologies. SCHOTT ranks number one in the world with many of its products. Its core markets are the household appliance, pharmaceutical, electronics, optics, and transportation industries. The company is strongly committed to contributing to its customers’ success and making SCHOTT an important part of people’s lives with high-quality products and intelligent solutions. SCHOTT is committed to managing its business in a sustainable manner and supporting its employees, society and the environment. The SCHOTT Group maintains close proximity to its customers with manufacturing and sales units in 35 countries. Its workforce of 15,400 employees generated worldwide sales of approximately 1.84 billion euros for the 2012/2013 fiscal year. SCHOTT AG, with its headquarters in Mainz (Germany) is owned by the Carl Zeiss Foundation.
Press contact:
Dr. Haike Frank
SCHOTT AG
Corporate Public Relations
Hattenbergstrasse 10, 55122 Mainz, Germany
Phone: +49 (0)6131 / 66-4088
E-mail: michael-matthias.mueller@schott.com
Internet: www.schott.com

SCHOTT’s manufacturing process for producing sealing glass paste for solid oxide fuel cells: The specialty glass needed is first manufactured in a glass melt and then ground into glass powder. It is then processed into a glass paste and applied to the sta
Press contact
SCHOTT AG
Dr. Haike Frank
PR Manager
PR Manager
Hattenbergstraße 10
55122 Mainz
Germany
55122 Mainz
Germany
Phone: +49 6131/66-4088
Further information
SCHOTT AG
Salvatore Ruggiero
Vice President Marketing and Communication
Vice President Marketing and Communication
Hattenbergstraße 10
55122 Mainz
Germany
55122 Mainz
Germany
Phone: +49 6131/66-4140