Technical Details of SCHOTT® Cavity Cap
Accurate, reliable, and highly customizable
Technical Details for SCHOTT
| Material | D 263® Family | MEMpax® | AF 32® eco | BOROFLOAT® 33 | 
|---|---|---|---|---|
| CTE (ppm/K) | 7.2 | 3.3 | 3.2 | 3.3 | 
| Technical Data – Window | |
|---|---|
| Luminous transmittance τvD65 at 0.3 mm | ~ 91.7 % | 
| Thickness (h1) | 0.1 – 1.1 mm | 
| AR coating (single-side/double-side) | on demand | 
| Technical Data – Spacer | |
|---|---|
| Spacer height (h2) | 0.2 – 3.3 mm | 
| Opening size (a, b) | variable; min. 0.3 mm | 
| Opening tolerances | < 20 μm (equiv. ± 10 μm) | 
| Dam width (d1, d2) | down to 0.5 mm | 
| Technical Data – Cap | |
|---|---|
| Cap size (L, W) | variable; min. 3 x 3 mm | 
| Cap size tolerance | ± 100 μm | 
| Cap height (h1+h2) | min. 0.3 mm | 
| Chipping (inner edge) | < 10 μm | 
| Chipping (diced outer edge) | < 100 μm | 
Bonding
- 
    Wafer-level hermetic laser bonding: high level of hermeticity. 
- 
    Minimal heat load: heat-affected zone of just a few micrometers. 
- 
    Additive-free: no adhesives or extra materials required. 
SCHOTT® Cavity Cap Materials
SCHOTT® Cavity Cap is available as:
- 
    D 263® T eco 
- 
    AF 32® eco 
- 
    MEMpax® 
- 
    BOROFLOAT® 
To find out more, please see the related materials on the overview page.