SCHOTT UTG® for foldable displays
SCHOTT has been pushing the physical boundaries of specialty glass for more than 130 years. Today, SCHOTT UTG® is at the heart of the foldable revolution in the consumer electronics market, and has been awarded with the Guiness World Record for the thinnest glass on Earth at an early stage of its development.Ultra-thin, ultra-flexible, ultra-strong
Current smartphones and other screen-based devices are highly robust. In addition, upcoming cutting edge devices are also foldable. These features demand new cover glasses combining a range of properties that push the material to the very edge of technical feasibility. For best protection in extremely challenging conditions, the glass needs to be ultra-thin and ultra-flexible, and it needs to ultra-strong at the same time.How SCHOTT UTG® is defining the future of foldables
Features for new design opportunities
SCHOTT UTG® is the world’s first ultra-thin, ultra-strong glass that can be processed in mass volume, providing extraordinary flexibility and an exceptionally small bending radius for global manufacturers. These unique physical properties offer designers the freedom to create groundbreaking new devices in the consumer electronics market.Small bending radius
With an achievable bending radius of less than 2 mm, SCHOTT UTG® is tailor-made for foldable devices, retaining its high strength and impact resistance under the most demanding conditions.
Ultra-thin and ultra-strong
Smartphones and other electronic devices need to be able to withstand the toughest situations our everyday life throws at them, so their cover glass needs to be tough. Since SCHOTT UTG® is suitable for chemical strengthening, it remains strong and durable for the lifetime of the product.
Mass production
SCHOTT UTG® is available around the world for mass production, with consistently high quality materials and robust physical properties.
SCHOTT’s unique down-draw process
With the down-draw process, a glass ribbon is simply pulled down – the faster the glass ribbon is drawn, the thinner the end product and the more challenging the production. In addition to seamless thickness adjustment, the process offers the advantage of the glass requiring no or less secondary slimming, thus eliminating the downstream etching processes that are harmful to the environment. Glass produced by the down-draw process also shines, with a low thickness variation and a flawless surface (surface roughness ~1 nm). The result is SCHOTT UTG® – glass thinner than a human hair.
-
Discover how we process the thinnest, most flexible glass in the SCHOTT UTG® portfolio.
-
Find out more about SCHOTT UTG® – ultra-thin, ultra-flexible, and ultra-unbelievable.
SCHOTT UTG® wins 2021 DIC Award
After winning the SID Component of the Year Award in May 2021, SCHOTT UTG® won a 2021 DIC Award for shaping the ultimate in consumer breakthrough mobile devices.