Product variants of DURAN®

DURAN® is available in different types, each with their own unique properties to optimize elements of their performance. Available as tubes, rods and capillaries, options include a jumbo dimension variant and extra mechanical resilience for demanding applications.
DURAN® in Jumbo Size

DURAN® in Jumbo Size

The world-famous DURAN® borosilicate glass tubing can be processed with an outer diameter of up to 465 mm – a world record! This jumbo-sized DURAN® retains the high quality and technical properties of smaller DURAN® tubing, so is ideal for large-scale glass apparatus constructions such as chemical reactors.
DURAN® in Jumbo Size

CHARACTERISTICS

Since jumbo-sized DURAN® glass tubing is manufactured using the same direct-draw process as standard DURAN® tubing, it offers the same strength, tight tolerances, chemical and electrical resistance, optical quality, and thermal shock resistance.

 

YOUR ADVANTAGES

  • High quality glass tubing with large outer diameter. 
  • Tight tolerances and high mechanical strength.
DURATAN®

DURATAN®

On average, this thermally prestressed variant of DURAN® offers a higher level of mechanical resistance than the regular DURAN® range. With impact and stress resistance more than doubled (on average), DURATAN® is ideal for highly challenging applications.
DURATAN®
DURATAN®
  • DURATAN®
  • DURATAN®
CHARACTERISTICS

High scratch resistance and strong light transmission properties also make this variant ideal for external use, and a fine break pattern improves the safety characteristics of the glass as it breaks in a less hazardous way.



YOUR ADVANTAGES


On average 2-3 times higher resistance to tensile stress and mechanical impact compared to DURAN®.
Fine break pattern, similar to tempered safety glass (ESG).
DURAN® is a registered trademark of the DWK Life Sciences GmbH.

Want to know more? Let's talk!

Whether you need more information, samples, a quote, or advice for a project, I would be delighted to talk to you

Product Management Team

Product Management Team

Technical Tubing
1 Step 1
2
3

* Required field

SCHOTT will only use your data to respond to your inquiry. For more information, please click here.