Does this match your preferences? Make a selection.

Technical Details of ARTISTA® and RIVULETTA®

Materials of the finest quality, a production method over a century old, and a range of size options mean that SCHOTT structured decorative glass is the superior choice for the home and office. 

Two structured glasses, one high standard

Flexible manufacturing options

The variety of treatment options for ARTISTA® and RIVULETTA® mean both can be processed into safety, laminated or insulating glass, which offers potential for thermal and sound insulation roles.

The finest materials

The high standard set by ARTISTA® and RIVULETTA® comes from a unique production process that results in the finest quality low-iron sheet glass. Structured on just one side, ARTISTA® and RIVULETTA® are both crystal clear, with fire-polished surfaces for a truly elegant finish.

Pioneering process

RIVULETTA® is made by the tried and tested Fourcault process, the first fully mechanised method for continual manufacture of sheet glass introduced in 1914. Yet SCHOTT’s future-facing expertise and cutting-edge plant ensures this is glass for the 21st century.

Variety of thicknesses

To meet a diverse array of customer requirements, ARTISTA® and RIVULETTA® are available in a wide range of thicknesses.

ARTISTA®

SCHOTT ARTISTA® extra-clear decorative glass can be processed in the same way as conventional glass – either as safety, laminated or insulation glass. This opens up a variety of additional functions, ranging from thermal to sound insulation.

ARTISTA® offers a number of application possibilities for both interior and exterior use:

  • As a full pane
  • In stained glass
  • As a fused glass
Nominal thickness Tolerance Dimensions*
2.75 mm ± 0.25 mm 1,000 x 1,500 mm
    1,600 x 1,500 mm
    2,100 x 1,500 mm
     
4.0 mm ± 0.25 mm 1,800 x 1,500 mm
    2,100 x 1,500 mm
    2,400 x 1,500 mm
   

2,700 x 1,500 mm

     
6.0 mm ± 0.50 mm 2,100 x 1,500 mm
    2,400 x 1,500 mm
    2,700 x 1,500 mm
     
8.0 mm ± 0.50 mm 2,100 x 1,500 mm
    2,400 x 1,500 mm
    2,700 x 1,500 mm
     
10.0 mm ± 0.50 mm 2,100 x 1,500 mm
    2,400 x 1,500 mm

* Other dimensions upon request

RIVULETTA®

Colorless and clear, RIVULETTA® has an elegant, timeless design. The structured glass is produced by the Fourcault process, first used by the glass industry in 1914. This was the first fully mechanized process for the continual manufacture of sheet glass and involves drawing molten glass through the Fourcault nozzle. This produces the distinctive appearance of machine-drawn glass with a certain thickness tolerance and wavy surface.

Thickness Tolerance Dimensions*
4.0 mm ± 0.25 mm 2,100 x 1,500 mm
    2,400 x 1,500 mm
    2,700 x 1,500 mm
     
6.0 mm ± 0.50 mm 2,100 x 1,500 mm
    2,400 x 1,500 mm
    2,700 x 1,500 mm
     
8.0 mm ± 0.50 mm 2,100 x 1,500 mm
    2,400 x 1,500 mm
    2,700 x 1,500 mm

* Other dimensions upon request

ETA

Glass produced by SCHOTT’s special Fourcault drawn-glass process isn’t covered by the usual glass standards. Therefore, products using this process are also not subject to automatic regulation. ETA (European Technical Assessment) now confirms that SCHOTT Fourcault glass meets the requirements of the standards EN 12150-2, EN 14179-2, EN 14449 and EN 1279-5.

ETA represents an independent, Europe-wide valid certificate of performance for SCHOTT Fourcault glass as both a base glass and a processed product (toughened safety glass, laminated safety glass, laminated glass and insulating glass units). Extensive material testing at an accredited testing institute confirm the certified product properties.

ETA 

ETA or abZ?

As part of European harmonization, the customary abZ (Germany’s national technical approval) is used only nationally when no European harmonized specifications are available. The ETA (European Technical Assessment) replaces the abZ for member states of the European Union.

The point of contact for both certifications is the Deutsches Institut für Bautechnik (DIBt – German Institute for Construction Technology). 

Customer benefits

Customers can be assured that SCHOTT Fourcault glass can be processed into standard construction products, such as toughened safety glass, laminated safety glass, laminated glass and insulating glass units, in accordance with standards and can be designated as such.

That means no more time-consuming documentation and approval procedures, and processing options can be clearly communicated to customers using familiar terminology.

Production process

ARTISTA® and RIVULETTA® are produced by the Fourcault process, the first fully mechanised process for the continual manufacture of sheet glass. In this process, molten glass is drawn through a Fourcault nozzle that produces the distinctive appearance of machine-drawn glass, with a certain thickness tolerance and wavy surface.

SCHOTT-Machine-drawn-glasses-Production 

The Fourcault process involves six different stages:

  1. Preparation of batch
  2. Fill in of batch
  3. Glass melting
  4. Up-draw process
  5. Cooling down
  6. Edge cutting

Want to know more? Let’s talk

Whether you need more information, samples, a quote, or advice for a project, we would be delighted to talk to you.

Contact us
Man in glasses in business office on phone while working on laptop_605x350.jpg