Technical Details of Ceramic Laser Phosphor Converters
Stable, tough, and efficient
For dynamic ceramic converter solutions we offer yellow and green phosphor material with following material properties:
Yellow (polished ring or ring segment)
| 225 µm* thickness | Yellow SYA35 | Yellow SYB35 | Yellow SYC35 | Yellow SWA40 |
|---|---|---|---|---|
| Phosphor conversion efficacy (lm/W) |
310 ± 20 | 325 ± 15 | 315 ± 15 | 260 ± 20 |
| Emission color coordinates (cx) | 0.413 ± 0.01 | 0.417 ± 0.005 | 0.432 ± 0.005 | 0.410 ± 0.01 |
| Emission color coordinates (cy) | 0.561 ± 0.01 | 0.560 ± 0.005 | 0.549 ± 0.005 | 0.562 ± 0.01 |
| Temperature damage threshold | > 250°C | > 250°C | > 250°C | > 250°C |
Green (polished ring or ring segment)
| 225 µm* thickness | Green SGA35 | Green SGB35 | Green SGF35 | Green SGG35 | Shifted Green GGB35 |
|---|---|---|---|---|---|
| Phosphor conversion efficacy (lm/W) |
330 ± 20 | 320 ± 20 | 280 ± 20 | 250 ± 20 | 325 ± 20 |
| Emission color coordinates (cx) | 0.337 ± 0.005 | 0.330 ± 0.01 | 0.324 ± 0.01 | 0.320 ± 0.01 | 0.300 ± 0.01 |
| Emission color coordinates (cy) | 0.591 ± 0.005 | 0.588 ± 0.01 | 0.584 ± 0.01 | 0.580 ± 0.01 | 0.588 ± 0.01 |
| Temperature damage threshold | > 250°C | > 250°C | > 250°C | > 250°C | > 250°C |
Our dynamic solutions are available in different geometries:
| OD88 | OD64 | OD49 | OD35 | |
|---|---|---|---|---|
| Outer diameter* (mm) | 88 | 64 | 49 | 35 |
| Inner diameter* (mm) | 74 | 50 | 35 | 25 |
| Thickness* (mm) | 0.2 | 0.2 | 0.2 | 0.2 |
| Shape O ring | Available | Available | Available | Available |
| Shape Segment / C ring | Customized | Customized | Customized | Customized |
*Please note that the above values are not guaranteed and may vary within certain tolerances. These tolerances and more details are available upon request.
SCHOTT offers a range of dynamic solutions with different emission colors. Details of emission color coordinates can be found on the datasheet in the download section or in the tables above.
How does this solution work for green or yellow light?
Color coordinates of yellow and green Ceramic Converter materials in the 1931/2° color space.
Emission spectrum of yellow and green converter materials
90% QE relative to room temperature
We are happy to provide spectral data to support your optical design upon request.
Static Solutions for Digital Projection
For static ceramic converter solutions suitable for digital projection we offer yellow and green phosphor materials with following properties:
Yellow (anti-reflection coated phosphor on heatspreader)
| 80 µm* die thickness | Yellow SYA35 | Yellow SYB35 | Yellow SYC35 | Yellow SWA40 |
|---|---|---|---|---|
| Phosphor conversion efficacy (lm/W) |
> 240 | > 250 | > 240 | > 200 |
| Phosphor conversion efficiency (W/W) |
> 50% | > 52% | > 50% | > 42% |
| Emission color coordinates (cx) | 0.411 ± 0.01 | 0.417 ± 0.01 | 0.430 ± 0.01 | 0.409 ± 0.01 |
| Emission color coordinates (cy) | 0.561 ± 0.01 | 0.557 ± 0.01 | 0.546 ± 0.01 | 0.559 ± 0.01 |
Green (anti-reflection coated phosphor on heatspreader)
| 80 µm* die thickness | Green SGA35 | Green SGB35 | Green SGF35 | Green SGG35 | Shifted Green GGB35 |
|---|---|---|---|---|---|
| Phosphor conversion efficacy (lm/W) |
> 280 | > 270 | > 240 | > 210 | > 260 |
| Phosphor conversion efficiency (W/W) |
> 59% | > 57% | > 51% | > 45% | > 57% |
| Emission color coordinates (cx) | 0.333 ± 0.01 | 0.326 ± 0.01 | 0.320 ± 0.01 | 0.316 ± 0.01 | 0.299 ± 0.01 |
| Emission color coordinates (cy) | 0.590 ± 0.01 | 0.587 ± 0.01 | 0.583 ± 0.01 | 0.578 ± 0.01 | 0.579 ± 0.01 |
| 100 µm* die thickness | Yellow SYB35 | Green SGA35 |
|---|---|---|
| Phosphor conversion efficacy (lm/W) |
> 280 | > 280 |
| Emission color coordinates (cx) | 0.417 ± 0.01 | 0.333 ± 0.01 |
| Emission color coordinates (cy) | 0.557 ± 0.01 | 0.590 ± 0.01 |
*Please note that the above values are not guaranteed and may vary within certain tolerances. These tolerances and more details are available upon request.
Notes:
- Emission spectrum defined by the power spectral density > 465 nm.
- Efficacy and efficiency specified for emission spectrum.
- Anti-reflection coated phosphor optimized for blue light normal incidence.
- Efficacy, efficiency and color coordinates measured with 60° incident angle of blue laser (449.5 nm) at low laser power.
- Emission is detected in normal direction.
Our static solutions are available in following geometries:
Heat spreader dimension (W x L x T in mm)*
- 20 x 20 x 4
Phosphor material dimension (W x L x T in mm)*
- 4 x 4 x 0.080
- 4 x 4 x 0.100
Customized formats and detailed drawings are available upon request.
How does this solution work for green or yellow light?
Color coordinates of green and yellow ceramic converter materials in the CIE 1931/2° color space.
Emission spectrum
Range shows different materials including SYA35, SYB35, SYC35, SWA40 and SGA35, SGB35, SGF35, SGG35, GGB35 and others.
Irradiance limit
Notes:
- Indicated irradiance limits are not based on measurements, but on validated numerical simulation, taking into account all properties of relevance. Accordingly, the values on this page may in no case be understood as technical product specifications, and are for general orientation purposes, only.
- The values apply for illumination by a 450 nm CW mode laser with tophat profile, and for good thermal contact of a heatspreader sized 20 x 20 x 4 to a heatsink at 30 °C.
- For safety reasons stay at least 20% below indicated irradiance limit.
The blue laser light applied via a dichroic mirror blocks residual blue light, that is reflected from the sample.
We are happy to provide spectral data to support your optical design upon request.
Static Solutions for Illumination
We offer three types of white static converter materials for correlated color temperatures (CCT) of 6,000 K and 5,000 K, respectively, to suit a wide range of applications.
White 6,000 K (anti-reflection coated phosphor on heatspreader)
| 150 µm* die thickness | White SWA40 | White RWA45 | White RWB50 |
|---|---|---|---|
| Phosphor conversion efficacy (lm/W) |
> 230 | > 225 | > 220 |
| Phosphor conversion efficiency (W/W) |
> 63% | > 62% | > 62% |
| Emission color coordinates (cx) | 0.4100 ± 0.007 | 0.4170 ± 0.007 | 0.4233 ± 0.007 |
| Emission color coordinates (cy) | 0.5603 ± 0.007 | 0.5555 ± 0.007 | 0.5514 ± 0.007 |
| White color coordinates (cx) | 0.3198 | 0.3205 | 0.3212 |
| White color coordinates (cy) | 0.3655 | 0.3546 | 0.3454 |
| Emission color coordinates (u’) | 0.1842 | 0.1889 | 0.1931 |
| Emission color coordinates (v’) | 0.5664 | 0.5661 | 0.5659 |
| White color coordinates (u’) | 0.1896 | 0.1938 | 0.1976 |
| White color coordinates (v’) | 0.4876 | 0.4825 | 0.4781 |
White 5,000 K (anti-reflection coated phosphor on heatspreader)
| 150 µm* die thickness | White SWD50 | White RWP55 | White RWQ60 |
|---|---|---|---|
| Phosphor conversion efficacy (lm/W) |
> 240 | > 235 | > 230 |
| Phosphor conversion efficiency (W/W) |
> 62% | > 61% | > 61% |
| Emission color coordinates (cx) | 0.4142 ± 0.007 | 0.4229 ± 0.007 | 0.4287 ± 0.007 |
| Emission color coordinates (cy) | 0.5598 ± 0.007 | 0.5533 ± 0.007 | 0.5490 ± 0.007 |
| White color coordinates (cx) | 0.3520 | 0.3500 | 0.3488 |
| White color coordinates (cy) | 0.4286 | 0.4063 | 0.3926 |
| Emission color coordinates (u’) | 0.1864 | 0.1924 | 0.1964 |
| Emission color coordinates (v’) | 0.5668 | 0.5663 | 0.5659 |
| White color coordinates (u’) | 0.1893 | 0.1951 | 0.1990 |
| White color coordinates (v’) | 0.5185 | 0.5096 | 0.5038 |
*Please note that the above values are not guaranteed and may vary within certain tolerances. These tolerances and more details are available upon request.
Tolerance window for white color coordinates (cx;cy) / (u’;v’) for download in the download section.
Notes:
- White color coordinates change with blue laser wavelength and are measured at 449.5 nm.
- Emission spectrum is defined by the power spectral density > 465 nm.
- Efficacy and efficiency is measured for full (white) spectrum, defined by the power spectral density > 400 nm.
- AR coating optimized for blue light incident angle of 60°.
- Efficacy, efficiency and color coordinates measured with 60° incident angle of blue laser at low laser power.
- Emission is detected in normal direction.
Our static solutions are available in following geometries:
Heat spreader dimension (W x L x T in mm)*
- 20 x 20 x 4
Phosphor material dimension (W x L x T in mm)*
- 4 x 4 x 0.150
Custom formats and detailed drawings are available upon request.
How does this solution work for white light?
Color coordinates of white ceramic converter materials in the CIE 1931/2° color space.
Emission spectrum
Irradiance limit
Notes:
- Indicated irradiance limits are not based on measurements, but on validated numerical simulation, taking into account all properties of relevance. Accordingly, the values on this page may in no case be understood as technical product specifications, and are for general orientation purposes, only.
- The values apply for illumination by a 450 nm CW mode laser with tophat profile, and for good thermal contact of a heatspreader sized 20 x 20 x 4 to a heatsink at 30 °C.
- For safety reasons stay at least 20 % below indicated irradiance limit.
To meet the desired color coordinates, the material is designed for diffuse reflection of just the right portion of blue light.
We are happy to provide spectral data to support your optical design upon request.