Please note: Due to maintenance the shop will be unavailable on Tuesday, July 08, from 06:00 AM until 08:00 AM (CEST)

LF5G19

Glass Code:  597399.330
SCHOTT Advanced Optics offers a variety of radiation resistant glass types with different dispersion properties. These glass types are well-suited to use in surroundings with high radioactivity.
optical glass klein 4zu3.jpg
Characteristics
nd 1.59655 νd 39.89
ne 1.60010 νe 39.60
nF-nC 0.014954 nF'-nC' 0.015153
Need help or a quote?
CONTACT OUR SUPPORT
Technical Details
Refractive Indices
Characteristics λ [nm]
n2,325.4 2,325.4 1.56416
n1,970.1 1,970.1 1.56890
n1,529.6 1,529.6 1.57419
n1,060.0 1,060.0 1.58045
nt 1,014.0 1.58125
ns 852.1 1.58477
nr 706.5 1.58970
nC 656.3 1.59214
nC' 643.8 1.59284
Characteristics λ [nm]
n632.8 632.8 1.59349
nD 589.3 1.59642
nd 587.6 1.59655
ne 546.1 1.60010
nF 486.1 1.60710
nF' 480.0 1.60799
ng 435.8 1.61578
nh 404.7 1.62330
ni 365.0
Characteristics λ [nm]
n334.1 334.1
n312.6 312.6
n296.7 296.7
n280.4 280.4
n248.3 248.3
Internal Transmittance
Characteristics λ [nm]
τ25/2500 2,500 0.200
τ25/2325 2,325 0.316
τ25/1970 1,970 0.707
τ25/1530 1,530 0.979
τ25/1060 1,060 0.998
τ25/700 700 0.993
τ25/660 660 0.987
τ25/620 620 0.983
τ25/580 580 0.977
τ25/546 546 0.966
τ25/500 500 0.934
τ25/460 460 0.832
τ25/436 436 0.612
τ25/420 420 0.350
τ25/405 405 0.090
τ25/400 400 0.040
τ25/390 390
τ25/380 380
τ25/370 370
τ25/365 365
τ25/350 350
τ25/334 334
τ25/320 320
τ25/310 310
τ25/300 300
τ25/290 290
τ25/280 280
τ25/270 270
τ25/260 260
τ25/250 250
Characteristics λ [nm]
τ10/2500 2,500 0.525
τ10/2325 2,325 0.631
τ10/1970 1,970 0.870
τ10/1530 1,530 0.992
τ10/1060 1,060 0.999
τ10/700 700 0.997
τ10/660 660 0.995
τ10/620 620 0.993
τ10/580 580 0.991
τ10/546 546 0.986
τ10/500 500 0.973
τ10/460 460 0.929
τ10/436 436 0.822
τ10/420 420 0.657
τ10/405 405 0.382
τ10/400 400 0.276
τ10/390 390 0.090
τ10/380 380
τ10/370 370
τ10/365 365
τ10/350 350
τ10/334 334
τ10/320 320
τ10/310 310
τ10/300 300
τ10/290 290
τ10/280 280
τ10/270 270
τ10/260 260
τ10/250 250
Partial Dispersion
Characteristics
Ps,t 0.2355
PC,s 0.4930
Pd,C 0.2946
Pe,d 0.2370
Pg,F 0.5803
Pi,h
P's,t 0.2324
P'C',s 0.5322
P'd,C' 0.2451
P'e,d 0.2339
P'g,F' 0.5139
P'i,h
Characteristics
ΔPC,t -0.0056
ΔPC,s -0.0028
ΔPF,e 0.0009
ΔPg,F 0.0036
ΔPi,g