RIVULETTA®

SCHOTT RIVULETTA® - extra clear structured glass is an exceptional white glass that is artfully manufactured. Smooth flowing, vertical lines are like clear flowing water. SCHOTT RIVULETTA® enables an elegant interplay of insights and privacy - ideal for timeless interiors that combine the openness of generous room design with a sense of privacy.

RIVULETTA®

Advantages:

  • Is made from extra-clear low-iron glass
  • Timeless, classic design
  • Has a fire-polished surface
  • Wide range of processing options
Sign in to choose your product

As a registered user in our shop you enjoy many advantages

  • Simply order
  • Stock overview
  • Simple profile management
Need help or a quote?
CONTACT OUR SUPPORT
Article Details
SCHOTT
Article
T
L
H
W
sqm.
Sides coated
Reflect. Color
Process. Opt.
Cont./Box (pcs.)
Cont./Box (sqm.)
 
 
 
 
 
 
 
 
 
 
 
 
 
 
 
 
 
 
 
 
 
 
 
 
 
 
 
 
 
 
 
 
 
 
 
Technical Details
General Description

SCHOTT Fourcault glasses: authentic, versatile, tested

RIVULETTA® is produced through the Fourcault process, that produces the distinctive appearance of machine-drawn glass with a certain thickness tolerance and wavy surface.

ETA (European Technical Assessment) confirms that SCHOTT Fourcault glass meets the requirements of the standards EN 12150-2, EN 14179-2, EN 14449 and EN 1279-5.

ETA English