SCHOTT® Microarray printing technology technical details
Microarray printing for manufacturability
Experience unmatched capacity and flexibility
Our proprietary non-contact Piezo printing technology
| Feature | Description |
|---|---|
| Drop volume | 30pL – 300pL single drop volumes Higher dispense volumes with stop-and-drop firing mode |
| Spot size range | 25µm – 150µm Higher spot sizes (up to 300µm) with stop-and-drop firing mode |
| Print mode |
|
| Print speed | Deposit of 32 unique biomaterial samples on every pass at a rate of 238 spots per second |
| Print tips | Up to 32 tips possible |
| Print type | Non-contact printing |
| Biomaterials | Dispensing a broad range of biomaterials (nucleic acids, proteins, complex antigens, peptides, etc.) in spotting buffers of varying composition and density |
| Substrates | Production of arrays on a wide range of substrate materials, including glass, polymer /plastic, or silicon, in standard or custom shapes and sizes |
| Batch sizes | Standard batch sizes are up to 136 standard microscope slides or 32 microtiter plate-sized glass |
Microarrays by material
Explore product variants
Explore product variants
Explore product variants
FAQs
Would you like to learn more about SCHOTT® Microarray printing technologies? Let’s talk!
Accelerate your vision and get to market faster!