Technical Details of Reed Switch Glass
Accuracy and consistency are our standard
Technology
The fabrication of glass tubes is one of SCHOTT's key competencies. All high-precision cutting equipment has been developed in-house. Key developments in recent years include a focus on reducing dimensional tolerances as well as miniaturization. Washing and packing in modern clean rooms enables excellent cleanliness and direct usability in our customers’ processes.
Specification
The following table details the properties of SCHOTT's 8516 Reed Glass:
| Glass Number | 8516 | 
|---|---|
| Sealing alloy | NiFe 52 | 
| Evaporation tendency 1) | 0 | 
| CTE 10-6/K | 8.9 | 
| Transformation temperature °C | 440 | 
| Softening point (107.6dPas) °C | 650 | 
| Working point (104dpas) °C | 990 | 
| Density g/cm3 | 2.56 | 
| Modulus of elasticity GPa | 72 | 
| Refractive index | 1.516 | 
| tk 100 (DIN 52326) °C | 250 | 
| Electrical volume resistivity (in cm) log ρ at 250 °C | 8.1 | 
| Electrical volume resistivity (in cm) log ρ at 350 °C | 6.4 | 
| Dielectric constant (25 °C, 1 MHz) | 6.5 | 
| Loss angle tanδ (25 °C, 1 MHz) | 25x10-4 | 
| Classes of chemical stability | |
| Transmission of 0.5 mm glass at 1.1 µm | 16 | 
| Water resistance (DIN 12111) class | 3 | 
| Acid resistance (DIN 12116) class | 1 | 
| Acid resistance (DIN 52322) class | 2 | 
Dimensions
Overview of available dimensions for IR tubes 8516*:
- Length from 7-50 mm**
| Outer Diameter | Inner Diameter | Wall Thickness | 
|---|---|---|
| 1.30 +/- 0.03 mm | 0.225 +/- 0.025 | |
| 1.45 +/- 0.05 mm | 0.225 +/- 0.025 | |
| 1.70 +/- 0.03 mm | 0.25 +/- 0.03 | |
| 1.75 +/- 0.03 mm | 0.25 +/- 0.03 | |
| 2.06 +/- 0.04 mm | 0.23 +/- 0.04 | |
| 2.10 +/- 0.05 mm | 0.275 +/- 0.025 | |
| 2.13 +/- 0.05 mm | 0.33 +/- 0.025 | |
| 2.15 +/- 0.04 mm | 0.28 +/- 0.04 | |
| 2.21 +/- 0.04 mm | 0.355 +/- 0.025 | |
| 2.40 +/- 0.05 mm | 1.71 +/- 0.05 mm | |
| 2.40 +/- 0.04 mm | 0.38 +/- 0.025 | |
| 2.40 +/- 0.05 mm | 0.32 +/- 0.05 | |
| 2.45 +/- 0.05 mm | 0.35 +/- 0.05 | |
| 2.50 +/- 0.025 mm | 2.0 +/- 0.025 mm | |
| 2.55 +/- 0.05 mm | 0.36 +/- 0.03 | |
| 3.00 +/- 0.05 mm | 2.20 +/- 0.05 mm | |
| 3.50 +/- 0.05 mm | 0.45 +/- 0.05 | |
| 3.85 +/- 0.05 mm | 0.33 +/- 0.03 | |
| 4.63 +/- 0.12 mm | 3.8 +/- 0.1 mm | |
| 4.90 +/- 0.07 mm | 3.7 +/- 0.07 mm | |
| 4.90 +/- 0.07 mm | 0.65 +/- 0.05 | |
| 4.90 +/- 0.10 mm | 0.55 +/- 0.05 | |
| 5.05 +/- 0.07 mm | 3.6 +/- 0.07 mm | |
| 5.10 +/- 0.10 mm | 0.65 +/- 0.05 | |
| 5.20 +/- 0.10 mm | 0.45 +/- 0.05 | |
| 6.50 +/- 0.10 mm | 0.56 +/- 0.05 | |
| 8.10 +/- 0.13 mm | 6.5 +/- 0.13 mm | 
*Subject to change. Other sizes available upon request. 
**Depending on the length-diameter ratio.
 