Technical Details
Internal Transmittance (Chart)
- SCHOTT
- S8851 - S8851
- Thickness
- 2.0
- Reflection factor
- 0.8800
Internal Transmittance (Table)
| λ [nm] | |
|---|---|
| 200 | |
| 210 | |
| 220 | |
| 230 | |
| 240 | |
| 250 | |
| 260 | |
| 270 | |
| 280 | |
| 290 | < 10⁻³ |
| 300 | 0.064 |
| 310 | 0.306 |
| 320 | 0.535 |
| 330 | 0.629 |
| 340 | 0.663 |
| 350 | 0.500 |
| 360 | 0.061 |
| 370 | 0.709 |
| 380 | 0.780 |
| 390 | 0.790 |
| 400 | 0.355 |
| 410 | 0.706 |
| 420 | 0.254 |
| 430 | 0.854 |
| 440 | 0.783 |
| 450 | < 10⁻³ |
| 460 | 0.038 |
| 470 | 0.431 |
| 480 | 0.571 |
| 490 | 0.605 |
| λ [nm] | |
|---|---|
| 500 | 0.922 |
| 510 | 0.828 |
| 520 | 0.818 |
| 530 | 0.571 |
| 540 | 0.113 |
| 550 | 0.605 |
| 560 | 0.969 |
| 570 | 0.668 |
| 580 | 0.323 |
| 590 | 0.487 |
| 600 | 0.861 |
| 610 | 0.981 |
| 620 | 0.974 |
| 630 | 0.813 |
| 640 | 0.235 |
| 650 | 0.341 |
| 660 | 0.587 |
| 670 | 0.936 |
| 680 | 0.947 |
| 690 | 0.972 |
| 700 | 0.994 |
| 710 | 0.998 |
| 720 | 0.988 |
| 730 | 0.865 |
| 740 | 0.546 |
| 750 | 0.548 |
| 760 | 0.792 |
| 770 | 0.939 |
| 780 | 0.932 |
| 790 | 0.761 |
| λ [nm] | |
|---|---|
| 800 | 0.505 |
| 810 | 0.581 |
| 820 | 0.830 |
| 830 | 0.940 |
| 840 | 0.983 |
| 850 | 0.983 |
| 860 | 0.900 |
| 870 | 0.832 |
| 880 | 0.792 |
| 890 | 0.793 |
| 900 | 0.793 |
| 910 | 0.775 |
| 920 | 0.754 |
| 930 | 0.735 |
| 940 | 0.721 |
| 950 | 0.728 |
| 960 | 0.728 |
| 970 | 0.634 |
| 980 | 0.601 |
| 990 | 0.798 |
| 1,000 | 0.896 |
| 1,010 | 0.926 |
| 1,020 | 0.946 |
| 1,030 | 0.950 |
| 1,040 | 0.922 |
| 1,050 | 0.829 |
| 1,060 | 0.671 |
| 1,070 | 0.537 |
| 1,080 | 0.525 |
| 1,090 | 0.648 |
| λ [nm] | |
|---|---|
| 1,100 | 0.759 |
| 1,110 | 0.798 |
| 1,120 | 0.814 |
| 1,130 | 0.772 |
| 1,140 | 0.679 |
| 1,150 | 0.608 |
| 1,160 | 0.662 |
| 1,170 | 0.705 |
| 1,180 | 0.674 |
| 1,190 | 0.605 |
| 1,200 | 0.507 |
| 1,250 | 0.558 |
| 1,300 | 0.885 |
| 1,350 | 0.582 |
| 1,400 | 0.625 |
| 1,450 | 0.565 |
| 1,500 | 0.636 |
| 1,550 | 0.719 |
| 1,600 | 0.851 |
| 1,650 | 0.940 |
| 1,700 | 0.983 |
| 1,750 | 0.980 |
| 1,800 | 0.952 |
| 1,850 | 0.808 |
| 1,900 | 0.538 |
| 1,950 | 0.299 |
| 2,000 | 0.515 |
| 2,050 | 0.636 |
| 2,100 | 0.840 |
| 2,150 | 0.961 |
| λ [nm] | |
|---|---|
| 2,200 | 0.971 |
| 2,250 | 0.958 |
| 2,300 | 0.909 |
| 2,350 | 0.840 |
| 2,400 | 0.777 |
| 2,450 | 0.730 |
| 2,500 | 0.698 |
| 2,550 | |
| 2,600 | |
| 2,650 | |
| 2,700 | |
| 2,750 | |
| 2,800 | |
| 2,850 | |
| 2,900 | |
| 2,950 | |
| 3,000 | |
| 3,050 | |
| 3,100 | |
| 3,150 | |
| 3,200 | |
| 3,250 | |
| 3,300 | |
| 3,350 | |
| 3,400 | |
| 3,450 | |
| 3,500 | |
| 3,550 | |
| 3,600 | |
| 3,650 | |
| λ [nm] | |
|---|---|
| 3,700 | |
| 3,750 | |
| 3,800 | |
| 3,850 | |
| 3,900 | |
| 3,950 | |
| 4,000 | |
| 4,050 | |
| 4,100 | |
| 4,150 | |
| 4,200 | |
| 4,250 | |
| 4,300 | |
| 4,350 | |
| 4,400 | |
| 4,450 | |
| 4,500 | |
| 4,550 | |
| 4,600 | |
| 4,650 | |
| 4,700 | |
| 4,750 | |
| 4,800 | |
| 4,850 | |
| 4,900 | |
| 4,950 | |
| 5,000 | |
| 5,050 | |
| 5,100 | |
| 5,150 | |
Optical values
| Reflection factor | |
|---|---|
| Pd | 0.880 |
| Reference thickness | |
|---|---|
| d [mm] | 2 |
| Refractive Indices n |
|---|
| nd (587.6 nm) = 1.678 |
Colorimetric evaluation
| Illuminant | A(Planck T = 2347K) | ||
|---|---|---|---|
| d [mm] | 1 | 2 | 3 |
| x | |||
| y | |||
| Y | |||
| λd [nm] | |||
| Pe | |||
| Illuminant | Planck T = 3200 K | ||
|---|---|---|---|
| d [mm] | 1 | 2 | 3 |
| x | |||
| y | |||
| Y | |||
| λd [nm] | |||
| Pe | |||
| Illuminant | D65 (TC = 6504 K) | ||
|---|---|---|---|
| d [mm] | 1 | 2 | 3 |
| x | |||
| y | |||
| Y | |||
| λd [nm] | |||
| Pe | |||
Physical values
| Density | |
|---|---|
| p [g/cm3] | 3.58 |
| Bubble content | |
|---|---|
| Bubble class | |
| Transformation temperature | |
|---|---|
| Tg [°C] | 659 |
| Temperature coefficient | |
|---|---|
| Tk [nm/°C] | |
| Chemical Resistance | |
|---|---|
| FR class | - |
| SR class | - |
| AR class | - |
| Thermal expansion | |
|---|---|
| α-30°C/+70°C [10-6/K] | |
| α20°C/300°C [10-6/K] | 7.18 |
| α20°C/200°C [10-6/K] | |