Technical Details
        
            Internal Transmittance (Chart)
        
- SCHOTT
- N-WG205 - N-WG205
- Thickness
- 2.0
- Reflection factor
- 0.9286
        
            Internal Transmittance (Table)
        
| λ [nm] | |
|---|---|
| 200 | 0.549 | 
| 210 | 0.639 | 
| 220 | 0.749 | 
| 230 | 0.838 | 
| 240 | 0.902 | 
| 250 | 0.945 | 
| 260 | 0.971 | 
| 270 | 0.983 | 
| 280 | 0.990 | 
| 290 | 0.994 | 
| 300 | 0.994 | 
| 310 | 0.995 | 
| 320 | 0.995 | 
| 330 | 0.997 | 
| 340 | 0.998 | 
| 350 | 0.999 | 
| 360 | 1.000 | 
| 370 | 0.999 | 
| 380 | 1.000 | 
| 390 | 0.999 | 
| 400 | 0.999 | 
| 410 | 1.000 | 
| 420 | 1.000 | 
| 430 | 1.000 | 
| 440 | 1.000 | 
| 450 | 1.000 | 
| 460 | 1.000 | 
| 470 | 1.000 | 
| 480 | 1.000 | 
| 490 | 1.000 | 
| λ [nm] | |
|---|---|
| 500 | 1.000 | 
| 510 | 1.000 | 
| 520 | 1.000 | 
| 530 | 1.000 | 
| 540 | 1.000 | 
| 550 | 1.000 | 
| 560 | 1.000 | 
| 570 | 1.000 | 
| 580 | 1.000 | 
| 590 | 1.000 | 
| 600 | 1.000 | 
| 610 | 1.000 | 
| 620 | 1.000 | 
| 630 | 1.000 | 
| 640 | 1.000 | 
| 650 | 1.000 | 
| 660 | 1.000 | 
| 670 | 1.000 | 
| 680 | 1.000 | 
| 690 | 1.000 | 
| 700 | 1.000 | 
| 710 | 1.000 | 
| 720 | 1.000 | 
| 730 | 1.000 | 
| 740 | 1.000 | 
| 750 | 1.000 | 
| 760 | 1.000 | 
| 770 | 1.000 | 
| 780 | 1.000 | 
| 790 | 1.000 | 
| λ [nm] | |
|---|---|
| 800 | 1.000 | 
| 810 | 1.000 | 
| 820 | 1.000 | 
| 830 | 1.000 | 
| 840 | 1.000 | 
| 850 | 1.000 | 
| 860 | 1.000 | 
| 870 | 1.000 | 
| 880 | 1.000 | 
| 890 | 1.000 | 
| 900 | 1.000 | 
| 910 | 1.000 | 
| 920 | 1.000 | 
| 930 | 1.000 | 
| 940 | 1.000 | 
| 950 | 1.000 | 
| 960 | 1.000 | 
| 970 | 1.000 | 
| 980 | 1.000 | 
| 990 | 1.000 | 
| 1,000 | 1.000 | 
| 1,010 | 1.000 | 
| 1,020 | 1.000 | 
| 1,030 | 1.000 | 
| 1,040 | 1.000 | 
| 1,050 | 1.000 | 
| 1,060 | 1.000 | 
| 1,070 | 1.000 | 
| 1,080 | 1.000 | 
| 1,090 | 1.000 | 
| λ [nm] | |
|---|---|
| 1,100 | 1.000 | 
| 1,110 | 1.000 | 
| 1,120 | 1.000 | 
| 1,130 | 1.000 | 
| 1,140 | 1.000 | 
| 1,150 | 1.000 | 
| 1,160 | 1.000 | 
| 1,170 | 1.000 | 
| 1,180 | 1.000 | 
| 1,190 | 1.000 | 
| 1,200 | 1.000 | 
| 1,250 | 1.000 | 
| 1,300 | 1.000 | 
| 1,350 | 1.000 | 
| 1,400 | 0.993 | 
| 1,450 | 0.999 | 
| 1,500 | 1.000 | 
| 1,550 | 1.000 | 
| 1,600 | 1.000 | 
| 1,650 | 1.000 | 
| 1,700 | 1.000 | 
| 1,750 | 1.000 | 
| 1,800 | 1.000 | 
| 1,850 | 1.000 | 
| 1,900 | 1.000 | 
| 1,950 | 0.998 | 
| 2,000 | 0.993 | 
| 2,050 | 0.993 | 
| 2,100 | 0.990 | 
| 2,150 | 0.969 | 
| λ [nm] | |
|---|---|
| 2,200 | 0.966 | 
| 2,250 | 0.969 | 
| 2,300 | 0.967 | 
| 2,350 | 0.952 | 
| 2,400 | 0.916 | 
| 2,450 | 0.912 | 
| 2,500 | 0.904 | 
| 2,550 | 0.886 | 
| 2,600 | 0.878 | 
| 2,650 | 0.865 | 
| 2,700 | 0.727 | 
| 2,750 | 0.165 | 
| 2,800 | 0.105 | 
| 2,850 | 0.128 | 
| 2,900 | 0.161 | 
| 2,950 | 0.199 | 
| 3,000 | 0.239 | 
| 3,050 | 0.282 | 
| 3,100 | 0.327 | 
| 3,150 | 0.369 | 
| 3,200 | 0.397 | 
| 3,250 | 0.389 | 
| 3,300 | 0.327 | 
| 3,350 | 0.220 | 
| 3,400 | 0.105 | 
| 3,450 | 0.034 | 
| 3,500 | 0.009 | 
| 3,550 | 0.002 | 
| 3,600 | < 10⁻³ | 
| 3,650 | < 10⁻³ | 
| λ [nm] | |
|---|---|
| 3,700 | 0.001 | 
| 3,750 | 0.003 | 
| 3,800 | 0.006 | 
| 3,850 | 0.006 | 
| 3,900 | 0.004 | 
| 3,950 | 0.003 | 
| 4,000 | 0.003 | 
| 4,050 | 0.003 | 
| 4,100 | 0.004 | 
| 4,150 | 0.004 | 
| 4,200 | 0.004 | 
| 4,250 | 0.003 | 
| 4,300 | 0.002 | 
| 4,350 | 0.001 | 
| 4,400 | < 10⁻³ | 
| 4,450 | < 10⁻³ | 
| 4,500 | < 10⁻³ | 
| 4,550 | < 10⁻³ | 
| 4,600 | < 10⁻³ | 
| 4,650 | < 10⁻³ | 
| 4,700 | < 10⁻³ | 
| 4,750 | < 10⁻³ | 
| 4,800 | < 10⁻³ | 
| 4,850 | < 10⁻³ | 
| 4,900 | < 10⁻³ | 
| 4,950 | < 10⁻³ | 
| 5,000 | < 10⁻³ | 
| 5,050 | < 10⁻³ | 
| 5,100 | < 10⁻³ | 
| 5,150 | < 10⁻³ | 
        
            Optical values
        
| Reflection factor | |
|---|---|
| Pd | 0.929 | 
| Reference thickness | |
|---|---|
| d [mm] | 2 | 
| Spectral values guaranteed | |
|---|---|
| λc (τi = 0.5) [nm] | 205 ± 10 | 
| Refractive Indices n | 
|---|
| nF (486.1 nm) = 1.481 | 
| nh (404.7 nm) = 1.489 | 
| ng (435.8 nm) = 1.485 | 
| ns (852.1 nm) = 1.470 | 
| ne (546.1 nm) = 1.478 | 
| nd (587.6 nm) = 1.476 | 
Colorimetric evaluation
| Illuminant | A(Planck T = 2347K) | ||
|---|---|---|---|
| d [mm] | 1 | 2 | 3 | 
| x | |||
| y | |||
| Y | |||
| λd [nm] | |||
| Pe | |||
| Illuminant | Planck T = 3200 K | ||
|---|---|---|---|
| d [mm] | 1 | 2 | 3 | 
| x | |||
| y | |||
| Y | |||
| λd [nm] | |||
| Pe | |||
| Illuminant | D65 (TC = 6504 K) | ||
|---|---|---|---|
| d [mm] | 1 | 2 | 3 | 
| x | |||
| y | |||
| Y | |||
| λd [nm] | |||
| Pe | |||
        
            Physical values
        
| Density | |
|---|---|
| p [g/cm3] | 2.22 | 
| Bubble content | |
|---|---|
| Bubble class | - | 
| Transformation temperature | |
|---|---|
| Tg [°C] | 440 | 
| Temperature coefficient | |
|---|---|
| Tk [nm/°C] | |
| Chemical Resistance | |
|---|---|
| FR class | - | 
| SR class | - | 
| AR class | - | 
| Thermal expansion | |
|---|---|
| α-30°C/+70°C [10-6/K] | |
| α20°C/300°C [10-6/K] | 4.1 | 
| α20°C/200°C [10-6/K] | |