SF56A

Glass Code:  785261.492

A classic glass type with lead oxide as an essential component for outstanding optical properties.

Find more information in the tabs below or on our website.

Compare glass types with our Interactive Abbe Diagram.

optical glass klein 4zu3.jpg
Characteristics
nd 1.78470 νd 26.08
ne 1.79180 νe 25.87
nF-nC 0.030092 nF'-nC' 0.030603
Sign in to choose your product

As a registered user in our shop you enjoy many advantages

  • Simply order
  • Stock overview
  • Simple profile management
Need help or a quote?
CONTACT OUR SUPPORT
Article Details
SCHOTT
Article
Glass type
L
W
T
DIA
Step
nd
Step
vd
nd
vd
Weight
 
Technical Details
Refractive Indices
Characteristics λ [nm]
n2,325.4 2,325.4 1.73406
n1,970.1 1,970.1 1.73925
n1,529.6 1,529.6 1.74559
n1,060.0 1,060.0 1.75473
nt 1,014.0 1.75606
ns 852.1 1.76220
nr 706.5 1.77136
nC 656.3 1.77605
nC' 643.8 1.77740
Characteristics λ [nm]
n632.8 632.8 1.77866
nD 589.3 1.78444
nd 587.6 1.78470
ne 546.1 1.79180
nF 486.1 1.80615
nF' 480.0 1.80800
ng 435.8 1.82449
nh 404.7 1.84092
ni 365.0
Characteristics λ [nm]
n334.1 334.1
n312.6 312.6
n296.7 296.7
n280.4 280.4
n248.3 248.3
Internal Transmittance
Characteristics λ [nm]
τ25/2500 2,500 0.700
τ25/2325 2,325 0.760
τ25/1970 1,970 0.920
τ25/1530 1,530 0.989
τ25/1060 1,060 0.997
τ25/700 700 0.995
τ25/660 660 0.993
τ25/620 620 0.994
τ25/580 580 0.994
τ25/546 546 0.994
τ25/500 500 0.989
τ25/460 460 0.974
τ25/436 436 0.950
τ25/420 420 0.900
τ25/405 405 0.760
τ25/400 400 0.680
τ25/390 390 0.410
τ25/380 380 0.100
τ25/370 370 0.010
τ25/365 365
τ25/350 350
τ25/334 334
τ25/320 320
τ25/310 310
τ25/300 300
τ25/290 290
τ25/280 280
τ25/270 270
τ25/260 260
τ25/250 250
Characteristics λ [nm]
τ10/2500 2,500 0.867
τ10/2325 2,325 0.896
τ10/1970 1,970 0.967
τ10/1530 1,530 0.996
τ10/1060 1,060 0.999
τ10/700 700 0.998
τ10/660 660 0.997
τ10/620 620 0.998
τ10/580 580 0.998
τ10/546 546 0.998
τ10/500 500 0.996
τ10/460 460 0.990
τ10/436 436 0.980
τ10/420 420 0.959
τ10/405 405 0.896
τ10/400 400 0.857
τ10/390 390 0.700
τ10/380 380 0.398
τ10/370 370 0.120
τ10/365 365 0.040
τ10/350 350
τ10/334 334
τ10/320 320
τ10/310 310
τ10/300 300
τ10/290 290
τ10/280 280
τ10/270 270
τ10/260 260
τ10/250 250
Partial Dispersion
Characteristics
Ps,t 0.2040
PC,s 0.4605
Pd,C 0.2874
Pe,d 0.2359
Pg,F 0.6098
Pi,h
P's,t 0.2006
P'C',s 0.4967
P'd,C' 0.2387
P'e,d 0.2319
P'g,F' 0.5390
P'i,h
Characteristics
ΔPC,t -0.0042
ΔPC,s -0.0032
ΔPF,e 0.0021
ΔPg,F 0.0098
ΔPi,g