Please note: Due to maintenance the shop will be unavailable on Tuesday, September 16, from 06:00 AM until 08:00 AM (CEST)

P-LASF47

Glass Code:  806409.454

"P" glass suitable for precision molding (low-Tg-glass).

Find more information in the tabs below or on our website.

Compare glass types with our Interactive Abbe Diagram.

optical glass klein 4zu3.jpg
Characteristics
nd 1.80610 νd 40.90
ne 1.81078 νe 40.66
nF-nC 0.019709 nF'-nC' 0.019941
Select product
€00.00
Need help or a quote?
CONTACT OUR SUPPORT
Article Details
SCHOTT
Article
Glass type
L
W
T
DIA
Step
nd
Step
vd
nd
vd
Weight
 
Technical Details
Refractive Indices
Characteristics λ [nm]
n2,325.4 2,325.4 1.76040
n1,970.1 1,970.1 1.76755
n1,529.6 1,529.6 1.77538
n1,060.0 1,060.0 1.78432
nt 1,014.0 1.78544
ns 852.1 1.79028
nr 706.5 1.79696
nC 656.3 1.80023
nC' 643.8 1.80116
Characteristics λ [nm]
n632.8 632.8 1.80203
nD 589.3 1.80593
nd 587.6 1.80610
ne 546.1 1.81078
nF 486.1 1.81994
nF' 480.0 1.82110
ng 435.8 1.83112
nh 404.7 1.84064
ni 365.0 1.85739
Characteristics λ [nm]
n334.1 334.1 1.87632
n312.6 312.6
n296.7 296.7
n280.4 280.4
n248.3 248.3
Internal Transmittance
Characteristics λ [nm]
τ25/2500 2,500 0.200
τ25/2325 2,325 0.530
τ25/1970 1,970 0.880
τ25/1530 1,530 0.981
τ25/1060 1,060 0.998
τ25/700 700 0.996
τ25/660 660 0.995
τ25/620 620 0.995
τ25/580 580 0.994
τ25/546 546 0.994
τ25/500 500 0.988
τ25/460 460 0.975
τ25/436 436 0.963
τ25/420 420 0.950
τ25/405 405 0.930
τ25/400 400 0.920
τ25/390 390 0.890
τ25/380 380 0.830
τ25/370 370 0.720
τ25/365 365 0.650
τ25/350 350 0.350
τ25/334 334 0.030
τ25/320 320
τ25/310 310
τ25/300 300
τ25/290 290
τ25/280 280
τ25/270 270
τ25/260 260
τ25/250 250
Characteristics λ [nm]
τ10/2500 2,500 0.525
τ10/2325 2,325 0.776
τ10/1970 1,970 0.950
τ10/1530 1,530 0.992
τ10/1060 1,060 0.999
τ10/700 700 0.998
τ10/660 660 0.998
τ10/620 620 0.998
τ10/580 580 0.998
τ10/546 546 0.998
τ10/500 500 0.995
τ10/460 460 0.990
τ10/436 436 0.985
τ10/420 420 0.980
τ10/405 405 0.971
τ10/400 400 0.967
τ10/390 390 0.954
τ10/380 380 0.928
τ10/370 370 0.877
τ10/365 365 0.842
τ10/350 350 0.657
τ10/334 334 0.250
τ10/320 320 0.012
τ10/310 310 0.000
τ10/300 300
τ10/290 290
τ10/280 280
τ10/270 270
τ10/260 260
τ10/250 250
Partial Dispersion
Characteristics
Ps,t 0.2459
PC,s 0.5049
Pd,C 0.2976
Pe,d 0.2376
Pg,F 0.5671
Pi,h 0.8502
P's,t 0.2430
P'C',s 0.5453
P'd,C' 0.2478
P'e,d 0.2348
P'g,F' 0.5025
P'i,h 0.8403
Characteristics
ΔPC,t 0.0117
ΔPC,s 0.0066
ΔPF,e -0.0021
ΔPg,F -0.0079
ΔPi,g -0.0482