N-LAF34

Glass Code:  773496.424

“N”-glass as an environmentally friendly alternative to conventional lead and arsenic-containing glass types.

Find more information in the tabs below or on our website.

Compare glass types with our Interactive Abbe Diagram.

optical glass klein 4zu3.jpg
Characteristics
nd 1.77250 νd 49.62
ne 1.77621 νe 49.38
nF-nC 0.015568 nF'-nC' 0.015719
Sign in to choose your product

As a registered user in our shop you enjoy many advantages

  • Simply order
  • Stock overview
  • Simple profile management
Need help or a quote?
CONTACT OUR SUPPORT
Article Details
SCHOTT
Article
Glass type
L
W
T
DIA
Step
nd
Step
vd
nd
vd
Weight
 
 
Technical Details
Refractive Indices
Characteristics λ [nm]
n2,325.4 2,325.4 1.73085
n1,970.1 1,970.1 1.73824
n1,529.6 1,529.6 1.74610
n1,060.0 1,060.0 1.75447
nt 1,014.0 1.75546
ns 852.1 1.75962
nr 706.5 1.76515
nC 656.3 1.76780
nC' 643.8 1.76855
Characteristics λ [nm]
n632.8 632.8 1.76924
nD 589.3 1.77236
nd 587.6 1.77250
ne 546.1 1.77621
nF 486.1 1.78337
nF' 480.0 1.78427
ng 435.8 1.79196
nh 404.7 1.79915
ni 365.0
Characteristics λ [nm]
n334.1 334.1
n312.6 312.6
n296.7 296.7
n280.4 280.4
n248.3 248.3
Internal Transmittance
Characteristics λ [nm]
τ25/2500 2,500 0.139
τ25/2325 2,325 0.449
τ25/1970 1,970 0.868
τ25/1530 1,530 0.973
τ25/1060 1,060 0.998
τ25/700 700 0.996
τ25/660 660 0.996
τ25/620 620 0.995
τ25/580 580 0.995
τ25/546 546 0.996
τ25/500 500 0.993
τ25/460 460 0.986
τ25/436 436 0.978
τ25/420 420 0.971
τ25/405 405 0.958
τ25/400 400 0.950
τ25/390 390 0.929
τ25/380 380 0.891
τ25/370 370 0.828
τ25/365 365 0.785
τ25/350 350 0.600
τ25/334 334 0.332
τ25/320 320 0.117
τ25/310 310 0.027
τ25/300 300
τ25/290 290
τ25/280 280
τ25/270 270
τ25/260 260
τ25/250 250
Characteristics λ [nm]
τ10/2500 2,500 0.454
τ10/2325 2,325 0.726
τ10/1970 1,970 0.945
τ10/1530 1,530 0.989
τ10/1060 1,060 0.999
τ10/700 700 0.998
τ10/660 660 0.998
τ10/620 620 0.998
τ10/580 580 0.998
τ10/546 546 0.998
τ10/500 500 0.997
τ10/460 460 0.994
τ10/436 436 0.991
τ10/420 420 0.988
τ10/405 405 0.983
τ10/400 400 0.980
τ10/390 390 0.971
τ10/380 380 0.955
τ10/370 370 0.927
τ10/365 365 0.908
τ10/350 350 0.815
τ10/334 334 0.643
τ10/320 320 0.424
τ10/310 310 0.236
τ10/300 300 0.069
τ10/290 290
τ10/280 280
τ10/270 270
τ10/260 260
τ10/250 250
Partial Dispersion
Characteristics
Ps,t 0.2674
PC,s 0.5256
Pd,C 0.3018
Pe,d 0.2382
Pg,F 0.5518
Pi,h
P's,t 0.2648
P'C',s 0.5679
P'd,C' 0.2515
P'e,d 0.2359
P'g,F' 0.4895
P'i,h
Characteristics
ΔPC,t 0.0126
ΔPC,s 0.0070
ΔPF,e -0.0023
ΔPg,F -0.0085
ΔPi,g