N-BAK4

Glass Code:  569560.305

“N”-glass as an environmentally friendly alternative to conventional lead and arsenic-containing glass types.

Find more information in the tabs below or on our website.

Compare glass types with our Interactive Abbe Diagram.

optical glass klein 4zu3.jpg
Characteristics
nd 1.56883 νd 55.98
ne 1.57125 νe 55.70
nF-nC 0.010162 nF'-nC' 0.010255
Sign in to choose your product

As a registered user in our shop you enjoy many advantages

  • Simply order
  • Stock overview
  • Simple profile management
Need help or a quote?
CONTACT OUR SUPPORT
Article Details
SCHOTT
Article
Glass type
L
W
T
DIA
Step
nd
Step
vd
nd
vd
Weight
 
 
Technical Details
Refractive Indices
Characteristics λ [nm]
n2,325.4 2,325.4 1.54044
n1,970.1 1,970.1 1.54561
n1,529.6 1,529.6 1.55111
n1,060.0 1,060.0 1.55688
nt 1,014.0 1.55755
ns 852.1 1.56034
nr 706.5 1.56400
nC 656.3 1.56575
nC' 643.8 1.56624
Characteristics λ [nm]
n632.8 632.8 1.56670
nD 589.3 1.56874
nd 587.6 1.56883
ne 546.1 1.57125
nF 486.1 1.57591
nF' 480.0 1.57649
ng 435.8 1.58149
nh 404.7 1.58614
ni 365.0 1.59415
Characteristics λ [nm]
n334.1 334.1
n312.6 312.6
n296.7 296.7
n280.4 280.4
n248.3 248.3
Internal Transmittance
Characteristics λ [nm]
τ25/2500 2,500 0.540
τ25/2325 2,325 0.710
τ25/1970 1,970 0.900
τ25/1530 1,530 0.982
τ25/1060 1,060 0.995
τ25/700 700 0.997
τ25/660 660 0.995
τ25/620 620 0.995
τ25/580 580 0.996
τ25/546 546 0.996
τ25/500 500 0.994
τ25/460 460 0.989
τ25/436 436 0.988
τ25/420 420 0.987
τ25/405 405 0.983
τ25/400 400 0.980
τ25/390 390 0.967
τ25/380 380 0.940
τ25/370 370 0.890
τ25/365 365 0.840
τ25/350 350 0.550
τ25/334 334 0.070
τ25/320 320
τ25/310 310
τ25/300 300
τ25/290 290
τ25/280 280
τ25/270 270
τ25/260 260
τ25/250 250
Characteristics λ [nm]
τ10/2500 2,500 0.782
τ10/2325 2,325 0.872
τ10/1970 1,970 0.959
τ10/1530 1,530 0.993
τ10/1060 1,060 0.998
τ10/700 700 0.999
τ10/660 660 0.998
τ10/620 620 0.998
τ10/580 580 0.998
τ10/546 546 0.998
τ10/500 500 0.998
τ10/460 460 0.996
τ10/436 436 0.995
τ10/420 420 0.995
τ10/405 405 0.993
τ10/400 400 0.992
τ10/390 390 0.987
τ10/380 380 0.976
τ10/370 370 0.954
τ10/365 365 0.933
τ10/350 350 0.787
τ10/334 334 0.345
τ10/320 320 0.012
τ10/310 310
τ10/300 300
τ10/290 290
τ10/280 280
τ10/270 270
τ10/260 260
τ10/250 250
Partial Dispersion
Characteristics
Ps,t 0.2749
PC,s 0.5321
Pd,C 0.3029
Pe,d 0.2383
Pg,F 0.5487
Pi,h 0.7879
P's,t 0.2724
P'C',s 0.5750
P'd,C' 0.2524
P'e,d 0.2361
P'g,F' 0.4869
P'i,h 0.7807
Characteristics
ΔPC,t -0.0034
ΔPC,s -0.0013
ΔPF,e -0.0001
ΔPg,F -0.0010
ΔPi,g -0.0087