Characteristics
nd 1.50137 νd 56.41
ne 1.50349 νe 56.15
nF-nC 0.008888 nF'-nC' 0.008967
Sign in to choose your product

As a registered user in our shop you enjoy many advantages

  • Simply order
  • Stock overview
  • Simple profile management
Need help or a quote?
CONTACT OUR SUPPORT
Article Details
SCHOTT
Article
Glass type
L
W
T
DIA
Step
nd
Step
vd
nd
vd
Weight
 
Technical Details
Refractive Indices
Characteristics λ [nm]
n2,325.4 2,325.4 1.47507
n1,970.1 1,970.1 1.48008
n1,529.6 1,529.6 1.48536
n1,060.0 1,060.0 1.49076
nt 1,014.0 1.49137
ns 852.1 1.49389
nr 706.5 1.49713
nC 656.3 1.49867
nC' 643.8 1.49910
Characteristics λ [nm]
n632.8 632.8 1.49950
nD 589.3 1.50129
nd 587.6 1.50137
ne 546.1 1.50349
nF 486.1 1.50756
nF' 480.0 1.50807
ng 435.8 1.51243
nh 404.7 1.51649
ni 365.0 1.52350
Characteristics λ [nm]
n334.1 334.1 1.53120
n312.6 312.6 1.53844
n296.7 296.7
n280.4 280.4
n248.3 248.3
Internal Transmittance
Characteristics λ [nm]
τ25/2500 2,500 0.520
τ25/2325 2,325 0.630
τ25/1970 1,970 0.850
τ25/1530 1,530 0.983
τ25/1060 1,060 0.996
τ25/700 700 0.997
τ25/660 660 0.994
τ25/620 620 0.993
τ25/580 580 0.993
τ25/546 546 0.992
τ25/500 500 0.991
τ25/460 460 0.990
τ25/436 436 0.988
τ25/420 420 0.988
τ25/405 405 0.987
τ25/400 400 0.986
τ25/390 390 0.982
τ25/380 380 0.973
τ25/370 370 0.966
τ25/365 365 0.958
τ25/350 350 0.910
τ25/334 334 0.720
τ25/320 320 0.310
τ25/310 310 0.130
τ25/300 300 0.020
τ25/290 290
τ25/280 280
τ25/270 270
τ25/260 260
τ25/250 250
Characteristics λ [nm]
τ10/2500 2,500 0.770
τ10/2325 2,325 0.831
τ10/1970 1,970 0.937
τ10/1530 1,530 0.993
τ10/1060 1,060 0.998
τ10/700 700 0.999
τ10/660 660 0.998
τ10/620 620 0.997
τ10/580 580 0.997
τ10/546 546 0.997
τ10/500 500 0.996
τ10/460 460 0.996
τ10/436 436 0.995
τ10/420 420 0.995
τ10/405 405 0.995
τ10/400 400 0.994
τ10/390 390 0.993
τ10/380 380 0.989
τ10/370 370 0.986
τ10/365 365 0.983
τ10/350 350 0.963
τ10/334 334 0.877
τ10/320 320 0.626
τ10/310 310 0.370
τ10/300 300 0.140
τ10/290 290
τ10/280 280
τ10/270 270
τ10/260 260
τ10/250 250
Partial Dispersion
Characteristics
Ps,t 0.2835
PC,s 0.5385
Pd,C 0.3037
Pe,d 0.2382
Pg,F 0.5475
Pi,h 0.7888
P's,t 0.2810
P'C',s 0.5817
P'd,C' 0.2531
P'e,d 0.2362
P'g,F' 0.4860
P'i,h 0.7819
Characteristics
ΔPC,t 0.0094
ΔPC,s 0.0041
ΔPF,e -0.0007
ΔPg,F -0.0015
ΔPi,g -0.0048