Spectral values guaranteed
λsi = 0.00001) [nm] 360
λci = 0.5) [nm] 420 ± 6
λp1i = 0.92) [nm] 530
Sign in to choose your product

As a registered user in our shop you enjoy many advantages

  • Simply order
  • Stock overview
  • Simple profile management
Need help or a quote?
CONTACT OUR SUPPORT
Article Details
SCHOTT
Article
Glass type
L
W
T
Weight
 
Technical Details
Internal Transmittance (Chart)

Only values between 1 and 30 with one decimal place are allowed.

SCHOTT
GG420 - GG420
Thickness
3.0
Reflection factor
0.9183
Internal Transmittance (Table)
λ [nm]
200 < 10⁻³
210 < 10⁻³
220 < 10⁻³
230 < 10⁻³
240 < 10⁻³
250 < 10⁻³
260 < 10⁻³
270 < 10⁻³
280 < 10⁻³
290 < 10⁻³
300 < 10⁻³
310 < 10⁻³
320 < 10⁻³
330 < 10⁻³
340 < 10⁻³
350 < 10⁻³
360 < 10⁻³
370 < 10⁻³
380 < 10⁻³
390 < 10⁻³
400 < 10⁻³
410 0.061
420 0.479
430 0.770
440 0.855
450 0.885
460 0.903
470 0.918
480 0.930
490 0.941
λ [nm]
500 0.950
510 0.958
520 0.964
530 0.970
540 0.975
550 0.978
560 0.981
570 0.983
580 0.984
590 0.985
600 0.986
610 0.986
620 0.986
630 0.985
640 0.985
650 0.984
660 0.983
670 0.983
680 0.981
690 0.980
700 0.979
710 0.978
720 0.977
730 0.975
740 0.974
750 0.972
760 0.971
770 0.969
780 0.968
790 0.966
λ [nm]
800 0.965
810 0.964
820 0.962
830 0.961
840 0.960
850 0.958
860 0.957
870 0.956
880 0.955
890 0.954
900 0.953
910 0.952
920 0.952
930 0.951
940 0.951
950 0.950
960 0.950
970 0.949
980 0.949
990 0.949
1,000 0.948
1,010 0.948
1,020 0.948
1,030 0.948
1,040 0.947
1,050 0.947
1,060 0.947
1,070 0.947
1,080 0.947
1,090 0.946
λ [nm]
1,100 0.946
1,110 0.946
1,120 0.946
1,130 0.947
1,140 0.947
1,150 0.947
1,160 0.947
1,170 0.947
1,180 0.947
1,190 0.947
1,200 0.947
1,250 0.948
1,300 0.950
1,350 0.953
1,400 0.952
1,450 0.958
1,500 0.963
1,550 0.966
1,600 0.969
1,650 0.970
1,700 0.970
1,750 0.970
1,800 0.968
1,850 0.966
1,900 0.965
1,950 0.963
2,000 0.961
2,050 0.959
2,100 0.956
2,150 0.950
λ [nm]
2,200 0.938
2,250 0.934
2,300 0.938
2,350 0.938
2,400 0.932
2,450 0.921
2,500 0.914
2,550 0.910
2,600 0.906
2,650 0.889
2,700 0.812
2,750 0.324
2,800 0.240
2,850 0.250
2,900 0.267
2,950 0.278
3,000 0.283
3,050 0.279
3,100 0.269
3,150 0.255
3,200 0.240
3,250 0.224
3,300 0.206
3,350 0.191
3,400 0.176
3,450 0.164
3,500 0.158
3,550 0.155
3,600 0.153
3,650 0.154
λ [nm]
3,700 0.157
3,750 0.164
3,800 0.172
3,850 0.177
3,900 0.179
3,950 0.174
4,000 0.166
4,050 0.155
4,100 0.141
4,150 0.123
4,200 0.105
4,250 0.086
4,300 0.066
4,350 0.046
4,400 0.024
4,450 0.009
4,500 0.003
4,550 < 10⁻³
4,600 < 10⁻³
4,650 < 10⁻³
4,700 < 10⁻³
4,750 < 10⁻³
4,800 < 10⁻³
4,850 < 10⁻³
4,900 < 10⁻³
4,950 < 10⁻³
5,000 < 10⁻³
5,050 < 10⁻³
5,100 < 10⁻³
5,150 < 10⁻³
Optical values
Reflection factor
Pd 0.918
Reference thickness
d [mm] 3
Spectral values guaranteed
λsi = 0.00001) [nm] 360
λci = 0.5) [nm] 420 ± 6
λp1i = 0.92) [nm] 530
Refractive Indices n
ns (852.1 nm) = 1.520
ne (546.1 nm) = 1.530
nd (587.6 nm) = 1.520
Colorimetric evaluation
Illuminant A(Planck T = 2347K)
d [mm] 1 2 3
x 0.450 0.453 0.455
y 0.410 0.412 0.414
Y 91 90 90
λd [nm] 581 581 581
Pe 0.04 0.07 0.10
Illuminant Planck T = 3200 K
d [mm] 1 2 3
x 0.426 0.429 0.432
y 0.403 0.405 0.408
Y 91 90 90
λd [nm] 579 579 579
Pe 0.04 0.07 0.10
Illuminant D65 (TC = 6504 K)
d [mm] 1 2 3
x 0.317 0.320 0.324
y 0.337 0.342 0.348
Y 91 90 89
λd [nm] 569 570 570
Pe 0.03 0.06 0.08
Physical values
Density
p [g/cm3] 2.55
Bubble content
Bubble class 3
Transformation temperature
Tg [°C] 535
Temperature coefficient
Tk [nm/°C] 0.07
Chemical Resistance
FR class 0
SR class 1.0
AR class 1.0
Thermal expansion
α-30°C/+70°C [10-6/K] 7.8
α20°C/300°C [10-6/K] 9