SCHOTT® low-loss
SCHOTT® low-loss glass is designed for advanced packaging applications. Its low dielectric constant supports broadband antenna solutions and high-frequency signal transmission. Combined with an extremely smooth surface and precise thickness control, it contributes to reliable performance in demanding communication applications.
Advanced performance for high-frequency applications
SCHOTT® low-loss glass offers exceptional properties for high-frequency applications, enabling - besides others - powerful and precise Antenna in Package (AIP) solutions. Its thermal expansion rate fulfills the exact needs of the semiconductor industry, ensuring seamless integration. The low alkaline content enhances its chemical stability, making SCHOTT® low-loss ideal also in harsh environment. It is also excellent for RF applications above 60GHz. Delivering minimal signal delay and outstanding efficiency, the glass performs reliably in demanding environments.