Technical Details of FLEXINITY®
Powerful, accurate and highly customizable
SCHOTT FLEXINITY® - Structured Glass Solutions
| Standard structuring capabilities* | |
|---|---|
| Thickness range (depending on glass type) | 0.1 – 3.3 mm | 
| Format | Max. 600 mm in diameter (round, square) | 
| Layout | Through structures according to customer specifications | 
| Structuring radius | Down to 25 μm | 
| Minimum dimension of structure element | 100 μm | 
| Feature size tolerance | < 20 μm (equiv. ± 10 μm) | 
| Wall taper angle | 90 ° ± 0.5 ° | 
| Edge exclusion zone | ≥ 3 mm | 
| Position tolerance of features | < 20 μm (equiv. ± 10 μm) | 
| Bridge width between structure elements | Down to 100 μm | 
*) limitations in feature design and demands deviating from these capabilities will be evaluated upon request
SCHOTT FLEXINITY® connect - Structured Glass Solutions
| Structures | |
|---|---|
| Thickness range (depending on glass type) | ~ 0.2 – 1.1 mm | 
| Structuring radius | 
            Down to 50 µm | 
| Format | Max. 600 mm in diameter (round, square) | 
| Position tolerance | Down to ± 3 µm* | 
| Amount of holes | Up to 1000 holes per sec* | 
| Layouts | |
| Structuring form | Round | 
| Position | Flexible | 
| Hole morphology | Straight | 
| Type | Through hole | 
| Material range** | |
| D 263® T eco, BOROFLOAT® 33, SCHOTT® AF 35 G | 
*) Depending on design
**) Other materials under evaluation
SCHOTT FLEXINITY® mini – Structured Glass Solutions
| Standard structuring capabilities* | |
|---|---|
| Thickness range (depending on glass type) | 0.1 – 3.3 mm | 
| Format (Frame) | Max. 600 mm in diameter | 
| Size of detached parts | Down to 1mm | 
| Layout (outer contour of detached parts) | Round, rectangular, free shape | 
| Layout (holes) | Through structures according to customer specifications | 
| Outer contour & hole radius | Down to 25 μm | 
| Minimum dimensions of structure elements | 100 μm | 
| Feature size tolerance | < 20 μm (equiv. ± 10 μm) | 
| Position tolerance of features | < 20 μm (equiv. ± 10 μm) | 
| Frame size | ≥ 10 mm | 
SCHOTT FLEXINITY® level – Structured Glass Solutions
| Standard structuring capabilities* | |
|---|---|
| Glass Types | D263® T Eco, BOROFLOAT® 33 | 
| Thickness range (depending on glass type) | 0.6 – 3.3 mm | 
| Format | Max. 600 mm in diameter (round, square) | 
| Layout | Non-through structures according to customer specifications;  can be combined with through structures*  | 
        
| Structuring radius | Down to 25 μm | 
| Minimum dimension of structure element | 100 μm | 
| Feature size tolerance | < 20 μm (equiv. ± 10 μm) | 
| Wall taper angle | 90 ° ± 0.5 ° | 
| Edge exclusion zone | ≥ 3 mm | 
| Position tolerance of features | < 20 μm (equiv. ± 10 μm) | 
| Ridge width between structure elements | Down to 100 μm | 
| Specifications FLEXINITY® level | |
|---|---|
| Level Depth range, d1 | Min. 0.2 mm* | 
| Remaining Base Thickness, d0 | Min. 0.4 mm* | 
| Layout cavity | Round, rectangular, free shape | 
| Feature size tolerance (lateral) | < 20 μm (equiv. ± 10 μm) | 
| Position tolerance of features | < 20 μm (equiv. ± 10 μm) | 
| Level Depth tolerance | < 100 μm (equiv. ± 50 μm) | 
| Level Depth surface texture | Matte | 
FLEXINITY® materials
SCHOTT FLEXINITY® is available as:
- D 263® T eco
 - D 263® bio
 - AF 32® eco
 - MEMpax®
 - BOROFLOAT®
 
To find out more, please see the related materials on the overview page.