Technical Data
| Technical Data of CoralPor® Nano-Porous Glasses | CoralPor® Nano-Porous Monoliths | CoralPor® Nano-Porous Powder | 
|---|---|---|
| Shape | Rods, Discs, Plates | Powder | 
| Average pore diameter | 4 – 10 nm | 4 – 400 nm | 
| Specific surface area | 100 – 170 m2/g | 7 – 130 m2/g | 
| Specific pore volume | 0.2 – 0.3 cm3/g | 0.4 – 2 cm3/g | 
Typical Pore Size Distribution
Production process of Nano-Porous Glasses
CoralPor® Macro-Porous Glasses
Technical Data
| Technical Data of CoralPor® Macro-Porous Glasses | CoralPor® Macro-Porous Monoliths | CoralPor® Macro-Porous Granulate | 
|---|---|---|
| Shape | Rods, Discs, Plates | Granulate | 
        
| Average pore diameter | typically 1-500 µm | typically 1-300 µm | 
| Pore diameter distribution | Dependent on customer request | Dependent on customer request | 
| Porosity in volume % | 10 – 80 % | 10 – 80 % | 