DURAN® Borosilicate glass tubing

Ever since it was invented by Otto Schott in 1887, DURAN® has set the standard for borosilicate glass tubing. It remains a leading material for laboratories, industry and architecture thanks to its strength, versatility, resistance and vast range of dimensions for a variety of worldwide applications.

DURAN® is a registered trademark of DWK Life Sciences GmbH.

Download technical specs
A range of DURAN® borosilicate glass tubing
Overview

    Shop Buy DURAN® glass tubing online

    Order DURAN® borosilicate glass tubing directly via the SCHOTT Tubing Online Shop.

    Certificates We are certified

    ISO 3585:1998, ASTM E438 Type I, ISO 9001, ISO 15378 GMP standards

    Info Tubing up to 465 mm

    From precision capillaries to world-record jumbo tubing
    A selection of DURAN® borosilicate glass tubes

    A true all-rounder

    DURAN® glass tubes, rods and capillaries can be processed in a wide variety of dimensions, with very tight geometric tolerances and high optical quality. Its high geometrical accuracy and outstanding transmission properties offer further advantages, and given its robust mechanical durability and thermal shock resistance, DURAN® remains highly effective in harsh environments.
    Two DURAN® borosilicate glass tubes

    Applications across the board

    While DURAN® has been the go-to glass for laboratory and industrial applications for many years, it can now be found playing an important role in numerous other areas, whether that’s in photobioreactors for the cultivation of algae, or in architecture, art and interior design.
    For demanding glass components, DURAN® glass tubing is our trusted standard, combining consistently high quality with availability in a wide range of dimensions.
    Technical details

    Technical details of DURAN®

    DURAN® is widely used across industry, science, architecture and the arts thanks to its impressively broad range of technical assets. While it’s strong, durable and reliable in its physical properties, it also has the transparency and light transmission for very different areas of application.

    Do you know that we are also able to upgrade our DURAN® glass tubing, rods, and capillaries? Thermal shock cutting, fire polishing, bending, joining of glass parts as well as sawing, grinding, drilling, or sandblasting are only some of our capabilities in our further processing portfolio.

    Hydrolytic Resistance

     

    DURAN® borosilicate glass 3.3 is highly resistant to water, neutral and acid solutions, strong acids and their compounds, as well as chlorine and organic substances.

    Hydrolytic resistance  
    Hydrolytic resistance (DIN ISO 719) Class HGB 1
    Acid resistance (DIN 12116) Class S 1
    Alkali resistance (DIN ISO 695) Class A 2

     

    Other characteristics      
    Density ρ at 25°C 2.23 g · cm-3 Poisson number μ 0.20
    Elasticity modulus E (Young's modulus) 63 · 103 N · mm-2 Stress-optical constant:
    (DIN 52 314) K
    4.0 · 10-6 mm2 · N-1
     

    DURAN® borosilicate glass 3.3 is the ideal base material for accurate volume measurement thanks to consistently stable transmission from UV-A into the IR range.

     

    graphic UV transparency  Graphic UV Block

     

    Transmissionskurve DURAN (8330).png

     

    Poisson number μ 0.20
    Stress-optical constant:
    (DIN 52 314) K
    4.0 · 10-6 mm2 · N-1

    Graphic thermal shock

     

    Ideal for applications in contact with fire or high temperatures due to high working temperatures and tolerance to thermal shock. 

    Temperature resistance and thermal expansion  
    Coefficient of mean
    linear thermal expansion
    α (20°C; 300°C) as per DIN ISO 7991
    3.3 · 10-6 K-1
    Transformation temperature Tg 525°C
    Glass temperature
    at viscosity η in dPA · s:
       1013 (annealing point)
       107,6 (softening point)
       104 (working point)


    560°C
    825°C
    1260°C
    Thermal conductivity λw at 90°C 1.2 W · m-1 · K-1

    Good electrical properties

     

    Excellent for high-voltage applications thanks to its good electrical insulating characteristics with high dielectric strength. 

    Electrical properties    
    Temperature for specific
    electrical resistance of
    108 Ω · cm (DIN 52 326) tk 100
      250°C
    Log of the electric volume
    resistivity (Ω · cm)

    at 250°C
    at 230°C

    8
    6.5
    Dielectric poperties
    (1 MHz, 25°C)

    dielectric constant ε
    dielectric loss factor tan δ

    4.6
    37 · 10-4

    FAQs

    DURAN® glass tubes are available in a wide range of dimensions. The standard portfolio includes outside diameters from 3 mm to 465 mm, wall thicknesses from 0.45 mm to 14 mm, and lengths from 600 mm to 10,000 mm. Not all combinations of outside diameter, wall thickness, and length are technically feasible. Custom dimensions are available upon request, subject to a technical feasibility review. Detailed dimension tables and tolerances for the standard portfolio are provided in the DURAN® brochure in the download section.


    Available tolerances depend on the tube dimensions, wall thickness, and manufacturing process. SCHOTT provides tight geometric tolerances and high dimensional accuracy for technical applications. Detailed information on diameter, wall thickness, and other manufacturing tolerances for the standard portfolio is available in the DURAN® brochure in the download section. For tolerances outside our standard portfolio, please contact us for individual technical consultation.


    Depending on their dimensions, DURAN® glass tubes are packed in cartons, bulk cartons, wooden crates, or on pallets. Packaging units vary according to tube diameter, wall thickness, and length. The minimum order quantity for our standard portfolio is one packaging unit. For products outside the standard portfolio, our sales team will be pleased to provide the applicable minimum order quantity. Information on standard packaging and available packaging units can be found in the DURAN® brochure or obtained directly from our sales team. Please contact us directly to discuss custom packaging solutions.


    Yes. SCHOTT can develop and manufacture custom DURAN® glass tubes beyond the standard portfolio. Custom dimensions, special geometries, and application-specific requirements are assessed as part of a technical feasibility review. Our experts support you from material selection through product development.

    DURAN® borosilicate glass 3.3 is approved for pressure equipment made of borosilicate glass 3.3 in accordance with DIN EN 1595. The permissible pressure load depends on the outside diameter, wall thickness, geometry, and operating conditions. SCHOTT provides calculation principles and technical support for the design of pressure applications.

    The pressure resistance of DURAN® borosilicate glass 3.3 depends on the outside diameter (OD), wall thickness (WT), and applied pressure (p). For straight, stress-free glass tubes with a uniform wall thickness and open ends, the following formulas may be used as a guide:

    • Pressure resistance (p):
      p = (WT × 140 bar) / (OD − WT)
    • Required wall thickness (WT):
      WT = (OD × p) / (140 bar + p)

    Where:

    • OD = outside diameter in mm
    • WT = wall thickness in mm
    • p = pressure in bar

    These calculations are based on recognized standards for pressure equipment made of borosilicate glass 3.3 and support the design of pressurized applications. Additional technical information, calculation principles, and application examples are available in the DURAN® brochure for technical glass tubing. Suitability for a specific pressure application must always be assessed based on the actual operating conditions and applicable regulations.

    SCHOTT provides technical material data for DURAN®, including thermal, physical, chemical, optical, and electrical properties. These include the coefficient of linear thermal expansion (3.3 × 10⁻⁶ K⁻¹), transformation temperature, light transmission, chemical resistance, and mechanical properties. Complete data are available in the technical data sheet in the download section.

    SCHOTT provides a range of technical documents, certificates, and compliance information for DURAN® and its manufacturing site. These include product-specific documentation, quality certificates, and available regulatory declarations. Current documents are available in the download section or upon request.

    SCHOTT documents production, inspection, and packaging data throughout the manufacturing process. All relevant quality and production information is archived and can be used for traceability purposes. For more information on batch-specific documentation or certificates, please contact our sales team.

    DURAN® glass tubing is used in a wide range of industrial and scientific applications. Typical uses include laboratory equipment, chemical processing systems, sight glasses, heat exchangers, photobioreactors, ozone generators, ventilation systems, and applications in architecture, design, and lighting. Its combination of high chemical resistance, transparency, and thermal resistance makes DURAN® a versatile material.

    The mechanical load capacity of glass tubing is determined primarily by its surface condition, geometry, wall thickness, processing, and operating conditions. Because glass is a brittle material, specific load limits must be assessed for each application. SCHOTT provides technical support for evaluating and designing application-specific solutions.

    DURAN® glass tubing is continuously monitored and inspected during production. In addition to automated measurements, samples are regularly taken and evaluated in the laboratory for chemical, physical, and visual properties. All relevant quality data are documented and archived.

    Our experts provide support with material selection, processing, product development, and technical feasibility. Together with you, we assess your application requirements and recommend suitable solutions from our glass portfolio.

    If you identify a quality deviation, please contact your designated SCHOTT representative or our sales team. To support prompt processing, please provide as much detail as possible about the application, batch, and observed issue.

    DURAN® borosilicate glass 3.3 offers excellent resistance to water, neutral solutions, acids, and many organic substances. This performance is confirmed by the following classifications:

    • Hydrolytic resistance in accordance with DIN ISO 719: HGB 1
    • Acid resistance in accordance with DIN ISO 12116: Class S1
    • Alkali resistance in accordance with DIN ISO 695: Class A2

    Hydrofluoric acid, hot phosphoric acid, and alkaline solutions may attack the glass surface, depending on concentration and temperature. Suitability for specific media should therefore be assessed for the intended application.

    DURAN® offers high light transmission from the UV-A range into the infrared spectral range. Actual transmission depends on wall thickness and wavelength. Detailed transmission curves for defined wall thicknesses are available in the DURAN® brochure.

    The standard length of DURAN® glass tubing is approximately 1,500 mm. Other lengths may be available upon request, depending on the dimensions and application. Custom lengths are subject to a technical feasibility review.

    Information on sustainability initiatives, environmental targets, and product-specific sustainability data is available upon request. The availability of product carbon footprint (PCF) data may vary depending on the glass type and manufacturing site.

    Downloads
    Download

    Downloads for DURAN®

    Quality assurance & certifications

    Find documents like SDS, RoHS, REACH, ISO standards and more with our advanced filter tool!

    Download certificates

    Want to know more? Let’s talk.

    Applications

    Applications of DURAN®

    The versatility and robust properties of DURAN® glass makes it suitable for a broad range of applications. It's widely used across many areas of Industry and science for its high chemical and heat resistance, versatility and mechanical strength, while its stylish looks make it a favorite of architects the world over.
    A scientist using DURAN® borosilicate glass tubing in a laboratory

    A champion in the laboratory

    DURAN® has been an outstanding name in laboratory glassware for many years thanks to its high chemical resistance, geometrical accuracy, and non-flammable nature at high temperatures, while retaining impressive levels of transparency.

    Learn more
    Tubular glass photobioreactor for algae cultivation with glass tubing from SCHOTT

    Photobioreactors

    Photobioreactors require glass apparatus with specific properties to facilitate the cultivation of algae in the fields of nutrition and cosmetics. DURAN® tubes, manifolds, u-bends and j-bends prove highly useful thanks to their strong, stable light transmission and thermal resistance.

    Learn more
    DURAN® borosilicate glass tubing used in industrial heat exchangers and condensers

    Heat exchangers and condensers

    The transfer of heat between two or more gases is key to a range of industrial processes, and DURAN® glass is highly suitable due to its outstanding thermal shock and corrosion resistance. A key fixture in power stations and petrochemical plants, heat exchangers and condensers can also be found in air-conditioning and refrigeration units, as well as sewage treatment plants.

    Lounge area with blue walls and modern glass chandelier

    Designer lamps and explosion-proof lighting

    Alongside its industrial and scientific applications, DURAN® provides designers with an elegant option for stylish interior lighting. Whether in tube or rod shape, its outstanding transparency and contemporary look make it ideal for the latest lamp designs, as well as more functional applications such as explosion-proof lighting.

    Learn more
    DURAN® borosilicate glass tubing used in industrial chemical plants

    The right chemistry

    The geometrical precision and high chemical resistance of DURAN® glass tubing make it a popular choice for the equipment used in industrial chemical plants. Its high resistance to corrosion caused by water, acids, saline solutions, alkaline solutions and organic substances give it the stability required for these harsh chemical environments.

    DURAN® borosilicate glass tubing with high heat resistance used in sight glasses

    Sight glasses for extreme conditions

    The operation of tanks or boilers can depend on sight glasses that enable observation of the liquid levels within. However, strong pressures and high temperatures require a glass with exceptional heat resistance and mechanical resilience, as well as stable properties to ensure reliable operation. DURAN® provides the solution to all these challenges.

    DURAN® borosilicate glass tubing used in exterior and interior architecture design

    Attractive and functional architecture

    The mechanically rugged nature of DURAN® means it can be used in architecture as an attractive and stylish feature in both exterior and interior designs. When combined with creative lighting, it can result in a truly stunning effect that doesn’t compromise on safety or functionality.

    Learn more
    DURAN PDP-Applications: Food Dispenser: HAWOS_Silos-Leer_Desktop_615x615.jpg

    Food dispensers

    DURAN® glass tubing is ideal for food dispensers, which are becoming increasingly popular in the retail environment and buffet settings. As well as glass tubing presenting the food attractively, its high geometrical accuracy offers tight tolerances that also make it suitable for the storage of liquids. Scratch resistant with easy cleaning, the glass is highly robust and suitable for direct contact with food (certified).

    Customer success

    Learn from the experiences of our customers and discover what successful partnerships with SCHOTT can achieve.
      Text Image Slider 01_voice of our customers

      Glass tubing for autonomous solar lighting

      Find out how the partnership between FlexSol Solutions and SCHOTT brought light into the darkness. Through innovation and expertise, it was possible to create a lightweight lantern that combines durability, functionality, and all-weather performance.
      FlexSol Solutions
      More information
      Text Image Slider 02

      Glass tubing for a colorful world

      Uwe Michael Schlitt, Managing Director of OLDUS GmbH in Bensheim, Germany, explains why DURAN® is ideal for paint-mixing machines, replacing steel with glass tubing for a transparent, abrasion-resistant, and durable solution.
      OLDUS GmbH
      More information
      Text Image Slider 03

      Glass tubing for LED signal lights

      Airport and wind farm signal lights are vital for the safe operation of runways and turbines all over the world, and are designed to last for at least 20 years. Find out why Finnish company Obelux uses DURAN® glass tubing for its LED beacon lighting.
      Obelux
      More information
      Text Image Slider 04

      Air freshener for old buildings

      Discover how the process of photocatalysis using DURAN® glass tubing can decompose undesirable gases. This can transform musty, foul-smelling rooms into clean and fresh desirable places to be.
      Triplan Umwelttechnik
      More information
      Product variants

      Product variants of DURAN®

      DURAN® is available in different types, each with their own unique properties to optimize elements of their performance. Available as tubes, rods and capillaries, options include a jumbo dimension variant and extra mechanical resilience for demanding applications.

      Finished DURAN® Laboratory Glassware

      Are you searching for ready-to-use labware items like bottles, flasks, test tubes, or volumetric glassware? If yes, please contact DWK Life Sciences.

        Text Image Slider 01_inside voice

        Why customers trust DURAN®

        What makes DURAN® special is not just its outstanding technical performance, it's the confidence it gives our customers. From research laboratories to industrial production facilities around the globe, DURAN® glass tubing stands for quality, consistency, and long-term reliability.
        Vera Deinlein
        Product Manager Technical Tubing
        Contact

        Want to know more? Let's talk!

        Whether you need more information, samples, a quote, or advice for a project, I would be delighted to talk to you.

        Product Management Team

        Product Management Team

        Technical Tubing
        1 Step 1
        2
        3

        * Required field

        SCHOTT will only use your data to respond to your inquiry. For more information, please click here.

        1 Step 1
        2
        3

        * Required field

        SCHOTT will only use your data to respond to your inquiry. For more information, please click here.

        Want to know more? Let's talk!

        Please send any questions or requests by using the contact form.