Outstanding optical qualities
SCHOTT's Light Guide Rods offer exceptional white light transmission. In addition, we are able to offer solutions for UV and NIR applications, and our portfolio offers a wide range of numerical apertures.
Chemical and mechanical stability
The PURAVIS® glass optical fibers used in our Light Guide Rods offer strong chemical and mechanical resistance, which makes them suitable for harsh environments such as autoclaving systems.
Heat resistance
Hot fused ends withstand temperatures up to 400°C, allowing SCHOTT Light Guide Rods to resist thermal shock even in challenging environments.
Lead-free
Our PURAVIS® fibers are produced without arsenic or antimony and do not contain lead.