Barium Heavy Flint
To use all shop functionalities please sign in or register
Filter
        
            Optical Glass
        
                Steps nd/νd
    
    
                
        
            Tolerances according to ISO 12123 for refractive index (0.5: ±0.0001; 1: ±0.0002; 2: ±0.0003; 3: ±0.0005) and Abbe number (0.5: ±0.1%; 1: ±0.2%; 2: ±0.3%; 3: ±0.5%)
        
                Refractive Index nd
    
    
                
        
            Refractive index at the yellow helium line at 587.5618 nm
        
                Refractive Index ne
    
    
                
        
            Refractive index at the green mercury line at 546.0740 nm
        
                Abbe Number νd
    
    
                
        
            Abbe number is a measure for the dispersion. It is calculated by νd=(nd-1)/(nF-nC)
        
                Abbe Number νe
    
    
                
        
            Abbe number is a measure for the dispersion. It is calculated by νe=(ne-1)/(nF-nC)
        
                Standard Dispersion nF - nC
    
    
                
        
            Standard dispersion results from the difference of the refractive indices nF-nC
        
                Principal Dispersion nF' - nC'
    
    
                
        
            Principal dispersion results from the difference of the refractive indices nF'-nC'
        
                Relative Partial Dispersion Pg,F
    
    
                
        
            The relative partial dispersion Pg,F of the spectral lines g and F is derived the equation Pg,F= (ng - nF)/(nF - nC).
        
                Deviation Of Relative Partial Dispersion ΔPg,F
    
    
                
        
            Deviation of the relative partial dispersion from the normal line between the g- and F-line
        
                Humidity Resistance Class CR
    
    
                
        
            Climate resistance is resistance to moisture in the air expressed in CR classes 1 (high) to 4 (low).
        
                Stain Resistance Class FR
    
    
                
        
            Stain resistance class in accordance with SCHOTT optical filter glass catalog.
        
                Acid Resistance Class SR
    
    
                
        
            Acid resistance class in accordance with ISO 8424.
        
                Alkali Resistance Class AR
    
    
                
        
            Alkali resistance class in accordance with ISO 10629.
        
                Phosphate Resistance Class PR
    
    
                
        
            Resistance to alkaline phosphate containing solutions according to ISO 9689 expressed in PR classes 1 (high) to 4 (low).
        
                Thermal Expansion α(-30/+70)
    
    
                
        
            Linear coefficient of thermal expansion in 10-6/K in the temperature range [-30°C to +70°C].
        
                Transformation Temperature Tg
    
    
                
        
            Transformation temperature in °C according to ISO 7884-8
        
                Temperature Viscosity T107.6
    
    
                
        
            Temperature of the glass in °C at which the glass has a viscosity of 107.6 dPa·s
        
                Density ρ
    
    
                
        
            Density in g/cm³
        
                Knoop Hardness HK[0.1/20]
    
    
                
        
            Knoop Hardness HK[0.1/20] in accordance with ISO 9385.