SCHOTT® Solar Glass sphere

SCHOTT® Solar Glass sphere is an ultra-thin, highly transparent solar cell cover glass for space and terrestrial photovoltaic applications in low-radiation environments. Available as a commercial off-the-shelf (COTS) solution, it combines stable optical transmission, UV protection and lightweight design with a cost-performance balance suited to application-specific requirements.

Lightweight protection for space and terrestrial photovoltaics

SCHOTT® Solar Glass sphere combines high optical transmission with ultra-thin glass dimensions for photovoltaic applications in low-radiation environments. Standard thicknesses from 30 to 145 µm support lightweight solar cell designs for space and terrestrial applications.

Manufactured using SCHOTT’s down-draw process, the glass features ultra-flat, fire-polished surfaces on both sides without additional polishing. Standard sheet formats of 680 × 510 mm, with other dimensions available on request, provide flexibility for different photovoltaic configurations.

Five satellites orbit above Earth, with blue oceans, coastlines, and clouds visible below.

High optical transmission in ultra-thin glass

Solar cell cover glass must transmit usable sunlight while helping protect sensitive photovoltaic components from environmental exposure. SCHOTT® Solar Glass sphere combines high and stable optical transmission with reduced UV transmittance, supporting photovoltaic performance in applications with lower radiation exposure.

Its ultra-thin dimensions help reduce weight, while fire-polished surfaces and high edge strength support the mechanical requirements of solar cell integration. Available thicknesses and formats allow the glass to be selected according to the specific photovoltaic design.

Close-up of a transparent ultra-thin glass sheet bent into a loop, illustrating the flexibility of thin solar cell cover glass.

One glass. Two photovoltaic environments.

Space photovoltaics

Satellite with deployed solar panels orbiting Earth, illustrating solar cell applications in space photovoltaics.

For cost-sensitive satellite applications in lower-radiation environments, SCHOTT® Solar Glass sphere combines high optical transmission with lightweight protection. Its ultra-thin dimensions and commercial off-the-shelf availability make it a suitable option for photovoltaic arrays where weight and cost efficiency are important design considerations.

Vehicle-integrated photovoltaics

Gray passenger car with solar panels integrated into the roof, illustrating vehicle-integrated photovoltaics (VIPV) for solar power generation.

Integrating solar cells into vehicle surfaces creates opportunities to generate electricity directly where it is needed. SCHOTT® Solar Glass sphere offers ultra-thin, highly transparent cover glass for lightweight photovoltaic designs, combining optical performance with mechanical strength for automotive solar applications.

Learn more

Technical details

Geometrical properties Solar Glass sphere
Thickness portfolio* in µm 145
100
70
50
30

* Other thicknesses on request

Optical properties Solar Glass sphere
Refractive index nd   1.5231
Edge wavelength λc (τ = 46 %) at t = 100 µm nm 308
Thermal properties Solar Glass sphere
Transformation temperature Tg in °C 557
CTE (coefficient of thermal expansion) α(20 °C; 300 °C) in 10-6 · K-1 7.2
Mechanical properties Solar Glass sphere
Density ρ in g/cm³ 2.51
Young's modulus E in kN/mm² 72.9
Poisson's ratio μ   0.21

Spectral transmittance of SCHOTT® Solar Glass sphere

Spectral transmittance curves of 100 µm thick SCHOTT® Solar Glass sphere before and after UV solarization, showing high optical transmission across the visible and near-infrared spectrum.
UV transmittance curves of 100 µm thick SCHOTT® Solar Glass sphere before and after UV solarization, showing a sharp increase in light transmission above approximately 300 nm.

Commercial off-the-shelf glass for cost-efficient photovoltaic designs

SCHOTT® Solar Glass sphere offers a cost-efficient COTS solution for photovoltaic applications in low-radiation environments. Combining high optical transmission with standard ultra-thin glass thicknesses, it provides an established material option for lightweight space and terrestrial photovoltaic designs.

FAQs

SCHOTT® Solar Glass sphere is an ultra-thin, highly transparent solar cell cover glass for space and terrestrial photovoltaic applications in low-radiation environments. It provides lightweight protection while maintaining high optical transmission, making it suitable for applications such as satellite solar arrays and vehicle-integrated photovoltaics.

SCHOTT® Solar Glass sphere is available as a commercial off-the-shelf (COTS) glass, offering a cost-efficient alternative for photovoltaic applications that do not require the radiation resistance of specialized high-radiation cover glass. It combines established material properties with standard thicknesses and sheet formats, supporting application-specific product selection.

Both variants provide ultra-thin, highly transparent cover glass for photovoltaic applications. SCHOTT® Solar Glass sphere is positioned as a cost-efficient COTS solution for lower-radiation environments, including selected space and terrestrial applications. SCHOTT® Solar Glass exos is designed for more demanding space environments requiring enhanced resistance to UV and high-energy particle radiation and offers ECSS-qualified configurations.

SCHOTT® Solar Glass sphere is available in standard thicknesses of 30, 50, 70, 100 and 145 µm. Thicknesses up to 1 mm may be available on request. Standard sheet formats of 680 × 510 mm are listed in the product information, with other dimensions available upon request.

SCHOTT® Solar Glass sphere combines high optical transmission with reduced UV transmittance. Its glass composition is designed to resist UV-induced solarization, helping limit changes in optical transmission over time. This supports stable optical performance in photovoltaic applications with lower radiation exposure.

Yes. SCHOTT® Solar Glass sphere is suitable for consideration in vehicle-integrated photovoltaic applications, where solar cells generate electricity directly on vehicle surfaces. Its ultra-thin dimensions, high optical transmission and mechanical properties support lightweight cover glass concepts. Suitability for a specific vehicle design and integration process should be evaluated individually.

SCHOTT® Solar Glass sphere is a toughenable glass with high mechanical strength and fire-polished surfaces. In addition to standard thicknesses and sheet formats, other dimensions and thicknesses may be available on request. Specific processing and delivery options should be confirmed with SCHOTT for the intended application.

Discuss your space or terrestrial photovoltaic application

Talk to SCHOTT’s specialists about the right glass thickness, sheet format and material properties for your photovoltaic design.

Man in glasses in business office on phone while working on laptop_330x190.jpg

1 Step 1
2
3

*Required field

SCHOTT will only use your data to respond to your inquiry. For more information, please click here.