SCHOTT® Solar Glass Solar cell cover glass
High-performance solar cell cover glass engineered for lasting protection – from terrestrial photovoltaics to demanding space missions.
Reliable, protective and built to last
A quick look at what makes SCHOTT® Solar Glass reliable, protective and built to last – see technical details below for the full picture.
Technical details of SCHOTT® Solar Glass
Explore the technical properties, available formats and applications of SCHOTT® solar cell cover glass for photovoltaic systems in space and on Earth. This section covers optical and mechanical performance, large-format ultra-thin glass, coatings and product-specific qualification status.
High optical transmission
SCHOTT® Solar Glass offers high optical transmission across the spectral ranges relevant to photovoltaic applications. Product-specific transmission curves provide detailed information on the optical properties of each glass variant. Selected variants are designed to resist solarization caused by UV and high-energy particle radiation, helping maintain optical performance under demanding environmental conditions.
Optical properties:
| Optical properties | Solar Glass 0787 | Solar Glass sphere | Solar Glass exos | |
|---|---|---|---|---|
| Refractive index nd | 1.5080 | 1.5231 | 1.5145 | |
| Edge wavelength λc (τ = 46 %) at t = 100 µm | nm | 332 | 308 | 344 |
Protection against radiation
Solar and ultraviolet radiation, as well as charged particles, can gradually degrade photovoltaic materials. Cerium-doped SCHOTT® Solar Glass variants are developed to support UV and radiation protection while maintaining the optical transmission required by the solar cell. Required glass thickness and variant depend on the application and mission profile.
Solarization stability
Prolonged exposure to charged particles and UV radiation can cause glass darkening over time. SCHOTT® Solar Glass is engineered to resist solarization and discoloration, maintaining optical clarity and stable transmission for consistent efficiency throughout its lifetime.
High surface quality
The uniform, fire-polished surface of SCHOTT® Solar Glass minimizes surface roughness while supporting high-precision bonding and coating processes.
AR coating for higher usable transmittance
Anti-reflective coatings reduce surface reflection losses, a proven approach used across SCHOTT's optical glass portfolio, including mgf2 optical coating solutions. Other coating solutions on request.
SCHOTT® Solar Glass is available as:
- Sheets
- Large-format sheets for SCHOTT® Solar Glass exos up to 2 × 1 m
- Cut-to-size substrates
- AR-coated substrates
Coating options are variant-specific; a coating for SCHOTT® Solar Glass exos is currently under development. See the product variants and technical documents for available thicknesses, formats and processing options
The following tables compare selected geometrical, thermal and mechanical properties of SCHOTT® Solar Glass 0787, sphere and exos.
| Geometrical properties | Solar Glass 0787 | Solar Glass sphere | Solar Glass exos | |
|---|---|---|---|---|
| Thickness portfolio | in µm | 150 | 150 | 150 |
| 125 | 100 | 100 | ||
| 100 | 70 | 50 | ||
| 75 | 50 | |||
| 30 | ||||
| Thermal properties | Solar Glass 0787 | Solar Glass sphere | Solar Glass exos | |
|---|---|---|---|---|
| Transformation temperature Tg | in °C | 568 | 557 | 557 |
| CTE (coefficient of thermal expansion) α(20 °C; 300 °C) | in 10-6 · K-1 | 8.5 | 7.2 | 6.9 |
| Mechanical properties | Solar Glass 0787 | Solar Glass sphere | Solar Glass exos | |
|---|---|---|---|---|
| Density ρ | in g/cm³ | 2.51 | 2.51 | 2.54 |
| Young's modulus E | in kN/mm² | 70.0 | 72.9 | 74.5 |
| Poisson's ratio μ | 0.22 | 0.21 | 0.218 | |
Handling large-format ultra-thin glass
Thinness alone does not determine how ultra-thin glass behaves during handling. Edge and surface condition, glass format, contact, support and movement all influence the mechanical conditions acting on the glass. The handling concept therefore needs to match the specific thickness, dimensions and application.
FAQs
Find answers to common questions about solar cell cover glass, product selection, available thicknesses and formats, qualification, and the handling and integration of large-format ultra-thin glass.
Product selection and qualification
Solar cell cover glass is a thin, optically transparent layer positioned directly above a photovoltaic cell or cell assembly. This specialized solar cell glass helps protect sensitive materials while transmitting the wavelengths used for power generation. It is not necessarily the same as solar panel cover glass, which often refers to the large front glass of a complete terrestrial solar module.
SCHOTT® Solar Glass 0787, sphere and exos address different application profiles. Selection depends on factors such as radiation and UV exposure, optical requirements, thickness and format, qualification status, and integration needs. The product variant section below provides a first comparison; project-specific selection should be discussed with SCHOTT.
Availability is variant-specific. SCHOTT® Solar Glass includes ultra-thin options down to 30 µm. SCHOTT® Solar Glass exos is available from 30 to 150 µm and in large formats up to 2 × 1 m. Confirm cut sizes, tolerances and delivery form for the intended project.
SCHOTT® Solar Glass 0787 is qualified according to ECSS-E-ST-20-08C. SCHOTT® Solar Glass exos is currently in ECSS qualification. Qualification status should always be checked for the specific product, thickness and intended application.
Handling large-format ultra-thin glass
Yes. Ultra-thin glass can be handled reliably when the handling conditions are appropriately controlled. Mechanical behavior depends on more than thickness alone. Edge and surface condition, glass dimensions, contact, support and movement all influence how the glass responds during handling. The handling concept therefore needs to be matched to the specific glass configuration and application.
Large-format ultra-thin glass requires a handling concept that considers support, edge contact, cleanliness, transport and downstream bonding or lamination. Requirements depend on the glass dimensions, thickness, cell architecture and production process. Discuss the integration sequence and project-specific handling needs with SCHOTT early in development.
Edges and surfaces form the mechanical starting condition of ultra-thin glass. Small edge defects, scratches or local surface damage can concentrate mechanical stress and may become starting points for crack initiation under load. Precise edge processing and fire-polished surfaces provide a controlled starting condition. Appropriate handling helps preserve this condition throughout subsequent processing.
Thickness and format need to be considered together. Reducing glass thickness lowers bending stiffness and allows the glass to deflect more readily. Sheet dimensions influence unsupported spans and how mechanical loads are distributed. The same glass thickness can therefore behave differently depending on its dimensions, support conditions and movement during handling.
Manual handling can be feasible when contact, support and movement are controlled for the specific glass configuration. Thickness and dimensions influence the appropriate approach, so a method suitable for one format may not be suitable for another. Project-specific handling conditions should be evaluated before implementation.
Ultra-thin glass can be considered for automated handling when the system controls contact, support and movement for the specific glass configuration. The appropriate automation concept depends on glass thickness, dimensions and the individual process. Grippers, suction systems and process parameters therefore require application-specific validation.
Packaging, storage and unpacking should preserve the defined condition of the glass before active handling begins. Support, restraint and relative movement need to remain controlled as the glass moves from transport packaging into the next process step. The appropriate concept depends on the glass thickness, dimensions, transport conditions and subsequent handling method.
Bonding and integration
Adhesive selection depends on the glass variant, solar cell architecture, processing conditions and environmental requirements of the application. UV transmission and thermal expansion behavior can influence the performance of the bonded assembly. SCHOTT can provide information on the relevant glass properties to support application-specific material selection and validation.
Downloads for SCHOTT® Solar Glass
Find key documents for the SCHOTT® Solar Glass portfolio in one place, including declarations of conformity, material data sheets and product information for the available glass variants.
Want to know more? Let's talk!
Whether you need more information, samples, a quote, or advice for a project, I would be delighted to talk to you.
Want to know more? Let's talk
Please send any questions or requests by using the contact form.