Battery Lids and Connectors
Specifications
Specifications
Lithium Primary Battery Covers | Lithium-Ion Battery Covers | SCHOTT MinicapsTM | Ultracapacitor/Aluminium Electrolyte Capacitor Covers | |
---|---|---|---|---|
Gas-tightness | 1 x 10-8 mbar x l/s | 1 x 10-8 mbar x l/s |
1 x 10-8 mbar x l/s | 1 x 10-8 mbar x l/s |
Electrical Isolation | 108Ω to 109Ω |
Small designs: 108Ω to 109Ω Large designs: 107Ω to 108Ω |
1010Ω |
Small designs: 108Ω to 109Ω Large designs: 107Ω to 108Ω |
Chemical resistance | Chemical resistance High, against wide range of standard electrolytes incl. LiSO2, LiSOCL2, LiMnO2 | High, against range of standard electrolytes |
High, against range of standard electrolytes | High, against range of standard electrolytes |
Temperature stability | High: from -65°C to + 150°C |
High: from -65°C to + 150°C |
High: from -40°C to + 150°C |
High: from -40°C to + 150°C |
Pressure tightness | Very high | High to very high, depending on dimension | 10 N to 100 N and more, depending on design | High to very high, depending on dimension |
Mechanical strength | Very high | High to very high, depending on dimension | 10 N to 100 N and more, depending on design | High to very high, depending on dimension |
Sealing material | Glass | Glass | Glass | Glass |
Pins | Steel, Nickel Iron Alloys | Aluminum, Copper, Steel, Nickel Iron Alloys | Stainless Steel/Nickel Alloy | Aluminum |
Lid | Steel, Stainless Steel | Aluminum, Stainless Steel | Stainless Steel | Aluminum, Copper |
Lifetime | Up to 25 years | Up to 25 years | Up to 25 years |
Up to 25 years |
Claire Buckwar