Ceramic Laser Phosphor Converters

Smart thinking, premium materials and superior design have resulted in Ceramic Laser Phosphor Converters that operate with unrivalled performance.

Stable, tough, efficient and eco-friendly

Color gamut

Yellow and green ceramic phosphor material comprehensively covers the visible color spectrum. For selected applications, white phosphor ceramic is also available.

Reliability and long lifetime

SCHOTT Ceramic Laser Phosphor Converters offer long lifetime and stable operation. Pure inorganic phosphor solutions enable operations at high temperature levels and exhibit exceptional heat conductivity.

High luminance

SCHOTT technology ensures superior illuminance. High efficacy allows high contrast and high light output.

Variable formats

SCHOTT Ceramic Laser Phosphor Converters are available in various formats such as rings, dies, different colors and different heat sink types for dynamic & static solutions.
Dynamic Solutions


For dynamic ceramic converter solutions we offer yellow and green phosphor material with following material properties:

  Yellow
Green
Phosphor conversion efficacy (lm/W) 325 ± 15 330 ± 20
Emission color coordinates (cx)  0.417 ± 0.005   0.337 ± 0.005
Emission color coordinates (cy)   0.560 ± 0.005  0.591 ± 0.005
Thermal quenching stability @ 170°C   > 89%   > 92%
Temperature damage threshold   > 250°C   > 250°C
Thermal conductivity in temp. range from 25°C to 200°C (W/m-K)  5-10 data on request
More data and detailed information are available in the brochure in the download section.

 

 

Our dynamic solutions are available in different geometries:

  OD88 OD64 OD49 OD35
Outer diameter (mm) 88  64 49  35 
Inner diameter (mm) 74  50  35 25
Thickness (mm) 0.2 0.2 0.2 0.2 
Shape O ring  Available  Available   Available  Available  
Shape C ring (angle)  300°/310°  300°/310°   300°/310°   300°/310° 
Shape Segment On demand On demand On demand On demand

 

 

SCHOTT offers a range of dynamic solutions with different emission colors. Details of emission color coordinates can be find on the datasheet in the download section or in the graphic below:

 

Color coordinates of yellow and green Ceramic Converter material in the 1931/2° color space. 

Ceramic Converter Dynamic Solution Emission Colors

     

Emission spectrum of yellow and green converter material.

Ceramic Converter Dynamic Solution Emission Spectrum

 

 

Static Solutions for Digital Projection
 

For static ceramic converter solutions suitable for digital projection we offer yellow and green phosphor material with following material properties:

  Yellow Green
Phosphor conversion efficacy (lm/W)
> 280 > 280
Emision color coordinates (cx) 0.417 ± 0.01 0.333 ± 0.01
Emission coordinates (cy) 0.557 ± 0.01  0.588 ± 0.01 
Irradiance limit (W/mm2)  Up to 50 Up to 50 

More data and detailed information are available in the brochure in the download section.

 

Our static solutions are available in following geometries:

Heat spreader dimension (W x L x T in mm)

  • 20 x 20 x 4

Phosphor material dimension (W x L x T in mm)

  • 4 x 4 x 0.150

Customized formats and detailed drawings are possible on request.

 

How does this solution work for green or yellow light?

Ceramic Converter Static Solution Emission Spectrum for Green and Yellow

Blue laser light is applied via a dichroic mirror. This also blocks residual blue light, that is reflected from the sample.

Ceramic Converter Static Solution Graphic

 

 

Color coordinates of yellow, green and white Ceramic Converter material in the CIE 1931/2° color space.

Ceramic Converter Static Solution Emission Colors

 * The entire white area can be addressed based on your requirements

 

 

 

 

Static Solutions for Illumination


White light is the next generation of design. Therefore we offer, besides our standard yellow and green, also white phosphor material with following material properties for static ceramic converter solutions particularly suitable for illumination: 


Yellow Green White (5000K) White (6000K)
Phosphor conversion efficacy (lm/W) > 280 > 280 > 250 > 250
Emission color coordinates (cx) 0.417 ± 0.01 0.333 ± 0.01 0.341 ± 0.02 0.324 ± 0.02
Emission color coordinates (cy) 0.557 ± 0.01 0.588 ± 0.01 0.392 ± 0.02 0.346 ± 0.02
Irradiance limit (W/mm2) Up to 50 Up to 50 Up to 50 Up to 50

More data and detailed information are available in the brochure in the download section.


Our static solutions are available in following geometries:

Heat spreader dimension (W x L x T in mm)

  • 20 x 20 x 4

Phosphor material dimension (W x L x T in mm)

  • 4 x 4 x 0.150

Customized formats are possible on request.

 

How does this solution work for white light?

Ceramic Converter Static Solution Emission Spectrum for White

For white light generation, the material is designed for diffuse reflection of just the right portion of blue light to meet the desired color coordinates.

Ceramic Converter Static Solution Graphic

  

 

Color coordinates of yellow, green and white Ceramic Converter material in the CIE 1931/2° color space.

Ceramic Converter Static Solution Emission Colors

 

 
 
 

No.  Year Title Authors Published in                         
[2] 2020 Static ceramic phosphor assemblies for high power high luminance SSL-light sources for digital projection and specialty lighting V. Hagemann, A. Seidl, G. Weidmann  Proc. SPIE 11302
[1] 2019 Ceramic phosphor wheels for high luminance SSL-light sources with >500W of laser power for digital projection  V. Hagemann, A. Seidl, G. Weidmann  Proc. SPIE 10940
 
 
 

Want to know more? Let's talk

Whether you need more information, samples, a quote, or advice for a project, we would be delighted to talk to you.

Get in touch
Man in glasses in business office on phone while working on laptop