SCHOTT® Solar Glass Solar cell cover glass

High-performance solar cell cover glass engineered for lasting protection – from terrestrial photovoltaics to demanding space missions.

Download technical specs
SCHOTT® Solar Cell Cover Glass-Picture-Space-Technologie-Satellit-4
Overview

    Certificates.svg Flight heritage and qualification

    SCHOTT combines established space photovoltaic expertise with an ECSS-qualified glass variant and ISO 9001 and ISO 14001-certified management systems.

    Award & innovation.svg Large UTG for advanced solar cells

    SCHOTT® Solar Glass exos offers 30–150 µm thicknesses and formats up to 2 × 1 m2 for advanced solar cell designs.

    Blue handshake icon representing partnership or agreement Handling ultra-thin glass

    From contact and support to movement, discover key considerations for reliable glass handling.

    *Required field

    SCHOTT will only use your data to respond to your inquiry. For more information, please click here.

    Satellite with deployed solar panels orbiting Earth, illustrating solar cell applications in space photovoltaics.

    Exceptional clarity for lasting photovoltaic performance

    SCHOTT® Solar Glass is specialty solar cell cover glass designed for photovoltaic applications. Positioned directly above the cell, it transmits usable light while helping protect sensitive cell layers and interfaces from environmental exposure. High optical transmittance supports efficient power generation, while variant-specific UV filtering and solarization resistance help maintain optical performance over time. The portfolio includes cover glass solutions for satellite and terrestrial photovoltaic applications.
    Transparent ultra-thin glass sheets in different sizes and curved shapes, illustrating flexible glass formats for solar cell cover glass applications.

    Engineered protection for demanding environments

    From launch vibration to desert heat, photovoltaic cover glass must withstand mechanical and thermal stress while supporting optical performance. Available in thicknesses down to 30 µm, SCHOTT® Solar Glass combines low weight with strength and durability. Fire-polished surfaces support optical quality and downstream processing, while robust edges support resistance to mechanical stress during handling, integration and launch. Variant-specific thermal expansion properties support matching with selected solar cell architectures, while cerium-doped glass compositions help address UV and radiation exposure.
    From established space solar cells to next-generation photovoltaic technologies, different applications demand different cover glass properties. SCHOTT offers tailored glass solutions to meet these requirements.
    Technical details

    Technical details of SCHOTT® Solar Glass

    Explore the technical properties, available formats and applications of SCHOTT® solar cell cover glass for photovoltaic systems in space and on Earth. This section covers optical and mechanical performance, large-format ultra-thin glass, coatings and product-specific qualification status.

    High optical transmission

    SCHOTT® Solar Glass offers high optical transmission across the spectral ranges relevant to photovoltaic applications. Product-specific transmission curves provide detailed information on the optical properties of each glass variant. Selected variants are designed to resist solarization caused by UV and high-energy particle radiation, helping maintain optical performance under demanding environmental conditions.

     

    Comparison of UV-A and visible light transmittance for SCHOTT® Solar Glass 0787, sphere and exos at 100 µm thickness, showing different UV cut-off characteristics.

     

    Optical properties:

    Optical properties Solar Glass 0787 Solar Glass sphere Solar Glass exos
    Refractive index nd   1.5080 1.5231 1.5145
    Edge wavelength λc (τ = 46 %) at t = 100 µm nm 332 308 344

     

    Protection against radiation

    Solar and ultraviolet radiation, as well as charged particles, can gradually degrade photovoltaic materials. Cerium-doped SCHOTT® Solar Glass variants are developed to support UV and radiation protection while maintaining the optical transmission required by the solar cell. Required glass thickness and variant depend on the application and mission profile.

     

    Solarization stability

    Prolonged exposure to charged particles and UV radiation can cause glass darkening over time. SCHOTT® Solar Glass is engineered to resist solarization and discoloration, maintaining optical clarity and stable transmission for consistent efficiency throughout its lifetime.

    High surface quality

    The uniform, fire-polished surface of SCHOTT® Solar Glass minimizes surface roughness while supporting high-precision bonding and coating processes.

     

    AR coating for higher usable transmittance

    Anti-reflective coatings reduce surface reflection losses, a proven approach used across SCHOTT's optical glass portfolio, including mgf2 optical coating solutions. Other coating solutions on request.

    SCHOTT® Solar Glass is available as:

    • Sheets
    • Large-format sheets for SCHOTT® Solar Glass exos up to 2 × 1 m
    • Cut-to-size substrates
    • AR-coated substrates

    Coating options are variant-specific; a coating for SCHOTT® Solar Glass exos is currently under development. See the product variants and technical documents for available thicknesses, formats and processing options

    The following tables compare selected geometrical, thermal and mechanical properties of SCHOTT® Solar Glass 0787, sphere and exos.

     

    Geometrical properties Solar Glass 0787 Solar Glass sphere Solar Glass exos
    Thickness portfolio in µm 150 150 150
    125 100 100
    100 70 50
    75 50  
      30  

     

    Thermal properties Solar Glass 0787 Solar Glass sphere Solar Glass exos
    Transformation temperature Tg in °C 568 557 557
    CTE (coefficient of thermal expansion) α(20 °C; 300 °C) in 10-6 · K-1 8.5 7.2 6.9

     

    Mechanical properties Solar Glass 0787 Solar Glass sphere Solar Glass exos
    Density ρ in g/cm³ 2.51 2.51 2.54
    Young's modulus E in kN/mm² 70.0 72.9 74.5
    Poisson's ratio μ   0.22 0.21 0.218

    Handling

    Handling large-format ultra-thin glass

    Thinness alone does not determine how ultra-thin glass behaves during handling. Edge and surface condition, glass format, contact, support and movement all influence the mechanical conditions acting on the glass. The handling concept therefore needs to match the specific thickness, dimensions and application.

    Mechanical integrity

    Ultra-thin glass can be handled reliably when the handling conditions are appropriately controlled. High edge strength and fire-polished surfaces provide a robust starting condition. The handling concept then needs to preserve that condition throughout subsequent processing.

    Packaging storage and unpacking

    Handling begins before the glass reaches the process. Packaging, transport, storage and unpacking should preserve the defined condition of the glass and control support, contact and movement throughout each transition.

    Contact support and movement

    Controlled handling starts with defined contact and support conditions. Contact determines where mechanical loads enter the glass, while support influences how those loads are distributed and how the sheet can deflect during movement.

    Thickness format and application

    Thickness and format need to be considered together. Thinner glass deflects more readily, while sheet dimensions influence unsupported spans and load distribution. The same thickness can therefore require different handling conditions depending on format, support and movement.
    Faqs

    FAQs

    Find answers to common questions about solar cell cover glass, product selection, available thicknesses and formats, qualification, and the handling and integration of large-format ultra-thin glass.

    Product selection and qualification

    Solar cell cover glass is a thin, optically transparent layer positioned directly above a photovoltaic cell or cell assembly. This specialized solar cell glass helps protect sensitive materials while transmitting the wavelengths used for power generation. It is not necessarily the same as solar panel cover glass, which often refers to the large front glass of a complete terrestrial solar module.

    SCHOTT® Solar Glass 0787, sphere and exos address different application profiles. Selection depends on factors such as radiation and UV exposure, optical requirements, thickness and format, qualification status, and integration needs. The product variant section below provides a first comparison; project-specific selection should be discussed with SCHOTT.

    Availability is variant-specific. SCHOTT® Solar Glass includes ultra-thin options down to 30 µm. SCHOTT® Solar Glass exos is available from 30 to 150 µm and in large formats up to 2 × 1 m. Confirm cut sizes, tolerances and delivery form for the intended project.

    SCHOTT® Solar Glass 0787 is qualified according to ECSS-E-ST-20-08C. SCHOTT® Solar Glass exos is currently in ECSS qualification. Qualification status should always be checked for the specific product, thickness and intended application.

    Handling large-format ultra-thin glass

    Yes. Ultra-thin glass can be handled reliably when the handling conditions are appropriately controlled. Mechanical behavior depends on more than thickness alone. Edge and surface condition, glass dimensions, contact, support and movement all influence how the glass responds during handling. The handling concept therefore needs to be matched to the specific glass configuration and application.

    Large-format ultra-thin glass requires a handling concept that considers support, edge contact, cleanliness, transport and downstream bonding or lamination. Requirements depend on the glass dimensions, thickness, cell architecture and production process. Discuss the integration sequence and project-specific handling needs with SCHOTT early in development.

    Edges and surfaces form the mechanical starting condition of ultra-thin glass. Small edge defects, scratches or local surface damage can concentrate mechanical stress and may become starting points for crack initiation under load. Precise edge processing and fire-polished surfaces provide a controlled starting condition. Appropriate handling helps preserve this condition throughout subsequent processing.

    Thickness and format need to be considered together. Reducing glass thickness lowers bending stiffness and allows the glass to deflect more readily. Sheet dimensions influence unsupported spans and how mechanical loads are distributed. The same glass thickness can therefore behave differently depending on its dimensions, support conditions and movement during handling.

    Manual handling can be feasible when contact, support and movement are controlled for the specific glass configuration. Thickness and dimensions influence the appropriate approach, so a method suitable for one format may not be suitable for another. Project-specific handling conditions should be evaluated before implementation.

    Ultra-thin glass can be considered for automated handling when the system controls contact, support and movement for the specific glass configuration. The appropriate automation concept depends on glass thickness, dimensions and the individual process. Grippers, suction systems and process parameters therefore require application-specific validation.

    Packaging, storage and unpacking should preserve the defined condition of the glass before active handling begins. Support, restraint and relative movement need to remain controlled as the glass moves from transport packaging into the next process step. The appropriate concept depends on the glass thickness, dimensions, transport conditions and subsequent handling method.

    Bonding and integration

    Adhesive selection depends on the glass variant, solar cell architecture, processing conditions and environmental requirements of the application. UV transmission and thermal expansion behavior can influence the performance of the bonded assembly. SCHOTT can provide information on the relevant glass properties to support application-specific material selection and validation.

    Downloads
    Download

    Downloads for SCHOTT® Solar Glass

    Find key documents for the SCHOTT® Solar Glass portfolio in one place, including declarations of conformity, material data sheets and product information for the available glass variants.

    Want to know more? Let’s talk.

    Applications

    Applications of SCHOTT® Solar Glass

    The cover glass products of SCHOTT® Solar Glass protect photovoltaic systems and optical components wherever light is converted into energy. From satellites in orbit to solar installations on Earth, this precision-engineered glass ensures clarity, protection and reliable performance under the toughest conditions.
    Satellite with deployed solar arrays orbiting Earth, illustrating space photovoltaic applications.

    Space photovoltaics

    In space, solar arrays face radiation, atomic oxygen and extreme temperature cycles that can quickly degrade performance. SCHOTT® Solar Glass protects photovoltaic cells from these effects, maintaining optical clarity and mechanical integrity. From cost-efficient SCHOTT® Solar Glass sphere to the proven SCHOTT® Solar Glass 0787 and the advanced SCHOTT® Solar Glass exos, the family offers tailored cover glass options for every orbital regime and mission requirement.

    Read more
    Close-up of a satellite solar array with photovoltaic cells and spacecraft components, illustrating space solar cell applications

    Optical solar reflectors

    Thermal management in spacecraft is vital, requiring precise temperature regulation and stable heat exchange. For effective control, a spacecraft depends on efficient thermo-optical surfaces. When coated with a reflective layer, SCHOTT® Solar Glass 0787 provides a highly effective thermo-optical surface, shielding against harmful solar radiation while enabling heat exchange through high emittance in the infrared range.

    Electric vehicle with solar panels integrated into its roof, illustrating vehicle-integrated photovoltaics (VIPV) for solar power generation

    Terrestrial photovoltaics

    Phasing out fossil fuels creates new opportunities for solar cell applications. For example, the shift from internal combustion engines to electric powertrains increases demand for photovoltaic cells that generate electricity directly where it’s needed. When integrated into a vehicle’s surface, these cells require a lightweight cover that remains strong, flexible, and highly transparent throughout the vehicle’s lifetime.

    Customer success

    Learn from the experiences of our customers and discover what successful partnerships with SCHOTT can achieve.
      Text Image Slider-01-Protecting power for space

      Protecting power for space: advanced cover glass for next-generation solar cells

      Developed in cooperation with AZUR SPACE Solar Power GmbH and funded by ESA: SCHOTT® Solar Glass exos protects the power source of satellites – ensuring consistent performance from LEO constellations to GEO missions.
      AZUR SPACE Solar Power GmbH and ESA
      Read more
      Product variants

      Product variants of SCHOTT® Solar Glass

      Available in a range of ultra-thin, adaptable formats to suit demanding integration needs – explore SCHOTT® Solar Glass 0787, sphere and exos to find the right thickness and format for your application.

      Contact

      Want to know more? Let's talk!

      Whether you need more information, samples, a quote, or advice for a project, I would be delighted to talk to you.

      Man in glasses in business office on phone while working on laptop_470x265.jpg

      1 Step 1
      2
      3

      *Required field

      SCHOTT will only use your data to respond to your inquiry. For more information, please click here.

      Want to know more? Let's talk

      Please send any questions or requests by using the contact form.