Technical Details of SCHOTT® Cavity Cap
Accurate, reliable, and highly customizable
Technical Details for SCHOTT
| Material | D 263® Family | MEMpax® | AF 32® | BOROFLOAT® 33 |
|---|---|---|---|---|
| CTE (ppm/K) | 7.2 | 3.3 | 3.2 | 3.3 |
| Technical Data – Window |
|
|---|---|
| Luminous transmittance τvD65 at 0.3 mm | ~ 91.7 % |
| Thickness (h1) | 0.1 – 1.1 mm |
| AR coating (single-side/double-side) | on demand |
| Technical Data – Spacer |
|
|---|---|
| Spacer height (h2) |
0.2 – 3.3 mm |
| Opening size (a, b) | variable; min. 0.3 mm |
| Opening tolerances | < 20 μm (equiv. ± 10 μm) |
| Dam width (d1, d2) | down to 0.5 mm |
| Technical Data – Cap | |
|---|---|
| Cap size (L, W) | variable; min. 3 x 3 mm |
| Cap size tolerance | ± 100 μm |
| Cap height (h1+h2) | min. 0.3 mm |
| Chipping (inner edge) | < 10 μm |
| Chipping (diced outer edge) | < 100 μm |
Bonding
-
Wafer-level hermetic laser bonding: high level of hermeticity.
-
Minimal heat load: heat-affected zone of just a few micrometers.
-
Additive-free: no adhesives or extra materials required.
SCHOTT® Cavity Cap Materials
SCHOTT® Cavity Cap is available as:
-
D 263® T
-
AF 32®
-
MEMpax®
-
BOROFLOAT®
To find out more, please see the related materials on the overview page.