Technical Details of Ceramic Laser Phosphor Converters

Smart thinking, premium materials and superior design have resulted in Ceramic Laser Phosphor Converters that operate with unrivalled performance.

Stable, tough, and efficient

Color gamut

Yellow and green ceramic phosphor material comprehensively covers the visible color spectrum. For selected applications, white phosphor ceramic is also available.

Reliability and long lifetime

SCHOTT Ceramic Laser Phosphor Converters offer long lifetime and stable operation. Pure inorganic phosphor solutions enable operations at high temperature levels and exhibit exceptional heat conductivity.

High luminance

SCHOTT technology ensures superior illuminance. High efficacy allows high contrast and high light output.

Variable formats

SCHOTT Ceramic Laser Phosphor Converters are available in various formats such as rings, dies, different colors and different heat sink types for dynamic & static solutions.
Dynamic solutions


For dynamic ceramic converter solutions we offer yellow and green phosphor material with following material properties:

Yellow (225 µm* thickness*, polished ring or ring segment)

Optical specifications Yellow SYA35 Yellow SYA35i Yellow SYB35 Yellow SYB35i Yellow SYC35 Yellow SYC15i Yellow SYF35i
Conversion efficacy [lm/W]
310 ± 20 330 ± 15 325 ± 15 335 ± 15 315 ± 15 325 ± 15 290 ± 15
Emission color coordinates cx 0.413 ± 0.01 0.413 ± 0.01 0.417 ± 0.005 0.417 ± 0.005 0.432 ± 0.005 0.432 ± 0.005 0.562 ± 0.01
Emission color coordinates cy 0.561 ± 0.01 0.561 ± 0.01 0.560 ± 0.005 0.560 ± 0.005 0.549 ± 0.005 0.549 ± 0.005 0.562 ± 0.01

Green (225 µm* thickness*, polished ring or ring segment)

Optical specifications Green SGA35 Green SGB35 Green SGF35 Green SGG35 Shifted Green GGB35
Conversion efficacy [lm/W]
330 ± 20 320 ± 20 280 ± 20 250 ± 20 325 ± 20
Emission color coordinates cx 0.337 ± 0.005 0.330 ± 0.01 0.324 ± 0.01 0.320 ± 0.01 0.300 ± 0.01
Emission color coordinates cy 0.591 ± 0.005 0.588 ± 0.01 0.584 ± 0.01 0.580 ± 0.01 0.588 ± 0.01

*Please note that the above values are not guaranteed and may vary within certain tolerances. These tolerances and more details are available upon request.


You can find further information in the product brochure.

Static solutions for digital projection


For static ceramic converter solutions suitable for digital projection we offer yellow and green phosphor materials with following properties:

Yellow (80 µm* die thickness*, anti-reflection coated phosphor on heatspreader)

Optical specifications Yellow SYA35 Yellow SYA15 Yellow SYB35 Yellow SYB15 Yellow SYC35 Yellow SYC15 Yellow SYF35 Yellow SYF15
Conversion efficacy [lm/W]
> 235 > 260 > 250 > 275 > 240 > 265 > 200 > 230
Conversion efficiency [W/W]
> 49% > 54% > 52% > 57% > 50% > 55% > 42% > 48%
Emission color coordinates cx 0.410 0.410 0.415 0.415 0.425 0.425 0.405 0.405
Emission color coordinates cy 0.561 0.561 0.560 0.560 0.555 0.555 0.561 0.561

Green (80 µm* die thickness*, anti-reflection coated phosphor on heatspreader)

Optical specifications Green SGA35 Green SGA15 Green SGB35 Green SGB15 Green SGF35 Green SGF15 Green SGG35 Green SGG15 Shifted Green GGB35 Shifted Green GGB15
Conversion efficacy [lm/W]
> 270 > 295 > 260 > 285 > 240 * > 210 * > 260 *
Conversion efficiency [W/W]
> 57% > 62% > 55% > 60% > 51% * > 45% * > 57% *
Emission color coordinates cx 0.330 0.330 0.326 0.326 0.317 * 0.314 * 0.297 *
Emission color coordinates cy 0.588 0.588 0.587 0.587 0.583 * 0.578 * 0.579 *

*Please note that the above values are not guaranteed and may vary within certain tolerances. These tolerances and more details are available upon request.


You can find further information in the product brochure.

Static solutions for illumination


80 µm* die thickness*, anti-reflection coated phosphor on heatspreader

  9,000 K 6,500 K
Optical specifications White SWE40 White SWA40
Conversion efficacy [lm/W]
> 180 > 200
Conversion efficiency [W/W]
> 56% > 62%
Emission color coordinates cx 0.4070 0.4050
Emission color coordinates cy 0.5590 0.5610
White color coordinates cx 0.2865 0.3100
White color coordinates cy 0.2965 0.3510

150 µm* die thickness*, anti-reflection coated phosphor on heatspreader

    6,000 K 5,000 K  
Optical specifications White SWA40 White RWB50 White SWD50 White RWQ60
Conversion efficacy [lm/W]
> 230 > 220 > 250 > 230
Conversion efficiency [W/W]
> 63% > 62% > 64% > 61%
Emission color coordinates cx 0.4070 0.4220 0.4115 0.4270
Emission color coordinates cy 0.5620 0.5525 0.5605 0.5505
White color coordinates cx 0.3195 0.3210 0.3515 0.3485
White color coordinates cy 0.3710 0.3470 0.4310 0.3940

*Please note that the above values are not guaranteed and may vary within certain tolerances. These tolerances and more details are available upon request.


You can find further information in the product brochure.

Want to know more? Let's talk