FOTURAN® II

SCHOTT FOTURAN® II is a photo-structurable glass produced in a continuous melting process to achieve outstanding homogeneity. After UV exposure and temperature processes, fine and uniform structures can be formed, which can be used in areas that require the characteristics of both glass-ceramics and fine structures.
Glass disc with etched patterns

Extremely fine, advanced structuring

FOTURAN® II is a photo-structurable glass, with areas crystallized by UV exposure and heat treatment able to be etched to produce exceptionally fine structuring with a high aspect ratio – in customized 3D forms if required. After a second exposure and tempering process, FOTURAN® II can also be transformed into an opaque glass-ceramic.

Scientist in a laboratory inspecting a glass wafer

Adaptable for semiconductor packaging

Finely structured FOTURAN® II substrates have a very useful role in semiconductor and packaging processes. Structuring can be achieved without the need for photo-resist and can be used with equipment commonly available in the semiconductor industry, minimizing the work and extra costs involved.

We are certified

We are both ISO 9001 and 14001 certified. Our glass is subjected to stringent quality inspection before shipping and the production of FOTURAN® II is constantly monitored at all stages. It also complies with EU-RoHS and EU-REACH standards.

Man holding a glass disc made of SCHOTT FOTURAN® II
News & Innovation stories

The miracle material

Discover the range of possibilities with the revolutionary SCHOTT FOTURAN® II.

Read More

Fairs and Events

Meet our experts between 1 - 3 September 2021 in Shenzhen, China where they will be exhibiting at the China International Optoelectronic Exposition (CIOE). They are looking forward to meeting you and having some vibrant discussions.

Next Event

SEP

1 - 3

China International Optoelectronic Exposition

Shenzhen, China

Want to know more? Let’s talk

Whether you need more information, samples, a quote, or advice for a project, we would be delighted to talk to you.

Get in touch
Man in glasses in business office on phone while working on laptop