SCHOTT® Solar Glass sphere
Lightweight protection for space and terrestrial photovoltaics
SCHOTT® Solar Glass sphere combines high optical transmission with ultra-thin glass dimensions for photovoltaic applications in low-radiation environments. Standard thicknesses from 30 to 145 µm support lightweight solar cell designs for space and terrestrial applications.
Manufactured using SCHOTT’s down-draw process, the glass features ultra-flat, fire-polished surfaces on both sides without additional polishing. Standard sheet formats of 680 × 510 mm, with other dimensions available on request, provide flexibility for different photovoltaic configurations.
High optical transmission in ultra-thin glass
Solar cell cover glass must transmit usable sunlight while helping protect sensitive photovoltaic components from environmental exposure. SCHOTT® Solar Glass sphere combines high and stable optical transmission with reduced UV transmittance, supporting photovoltaic performance in applications with lower radiation exposure.
Its ultra-thin dimensions help reduce weight, while fire-polished surfaces and high edge strength support the mechanical requirements of solar cell integration. Available thicknesses and formats allow the glass to be selected according to the specific photovoltaic design.
Key advantages
One glass. Two photovoltaic environments.
Space photovoltaics
For cost-sensitive satellite applications in lower-radiation environments, SCHOTT® Solar Glass sphere combines high optical transmission with lightweight protection. Its ultra-thin dimensions and commercial off-the-shelf availability make it a suitable option for photovoltaic arrays where weight and cost efficiency are important design considerations.
Vehicle-integrated photovoltaics
Integrating solar cells into vehicle surfaces creates opportunities to generate electricity directly where it is needed. SCHOTT® Solar Glass sphere offers ultra-thin, highly transparent cover glass for lightweight photovoltaic designs, combining optical performance with mechanical strength for automotive solar applications.
Technical details
| Geometrical properties | Solar Glass sphere | |
|---|---|---|
| Thickness portfolio* | in µm | 145 |
| 100 | ||
| 70 | ||
| 50 | ||
| 30 | ||
* Other thicknesses on request
| Optical properties | Solar Glass sphere | |
|---|---|---|
| Refractive index nd | 1.5231 | |
| Edge wavelength λc (τ = 46 %) at t = 100 µm | nm | 308 |
| Thermal properties | Solar Glass sphere | |
|---|---|---|
| Transformation temperature Tg | in °C | 557 |
| CTE (coefficient of thermal expansion) α(20 °C; 300 °C) | in 10-6 · K-1 | 7.2 |
| Mechanical properties | Solar Glass sphere | |
|---|---|---|
| Density ρ | in g/cm³ | 2.51 |
| Young's modulus E | in kN/mm² | 72.9 |
| Poisson's ratio μ | 0.21 | |
FAQs
SCHOTT® Solar Glass sphere is an ultra-thin, highly transparent solar cell cover glass for space and terrestrial photovoltaic applications in low-radiation environments. It provides lightweight protection while maintaining high optical transmission, making it suitable for applications such as satellite solar arrays and vehicle-integrated photovoltaics.
SCHOTT® Solar Glass sphere is available as a commercial off-the-shelf (COTS) glass, offering a cost-efficient alternative for photovoltaic applications that do not require the radiation resistance of specialized high-radiation cover glass. It combines established material properties with standard thicknesses and sheet formats, supporting application-specific product selection.
Both variants provide ultra-thin, highly transparent cover glass for photovoltaic applications. SCHOTT® Solar Glass sphere is positioned as a cost-efficient COTS solution for lower-radiation environments, including selected space and terrestrial applications. SCHOTT® Solar Glass exos is designed for more demanding space environments requiring enhanced resistance to UV and high-energy particle radiation and offers ECSS-qualified configurations.
SCHOTT® Solar Glass sphere is available in standard thicknesses of 30, 50, 70, 100 and 145 µm. Thicknesses up to 1 mm may be available on request. Standard sheet formats of 680 × 510 mm are listed in the product information, with other dimensions available upon request.
SCHOTT® Solar Glass sphere combines high optical transmission with reduced UV transmittance. Its glass composition is designed to resist UV-induced solarization, helping limit changes in optical transmission over time. This supports stable optical performance in photovoltaic applications with lower radiation exposure.
Yes. SCHOTT® Solar Glass sphere is suitable for consideration in vehicle-integrated photovoltaic applications, where solar cells generate electricity directly on vehicle surfaces. Its ultra-thin dimensions, high optical transmission and mechanical properties support lightweight cover glass concepts. Suitability for a specific vehicle design and integration process should be evaluated individually.
SCHOTT® Solar Glass sphere is a toughenable glass with high mechanical strength and fire-polished surfaces. In addition to standard thicknesses and sheet formats, other dimensions and thicknesses may be available on request. Specific processing and delivery options should be confirmed with SCHOTT for the intended application.
Discuss your space or terrestrial photovoltaic application
Talk to SCHOTT’s specialists about the right glass thickness, sheet format and material properties for your photovoltaic design.