Product Variants of SCHOTT RealView®

SCHOTT serves augmented and mixed reality innovators worldwide as the leading provider of substrates for the waveguides in smart glasses or head-mounted devices. For all technologies within the industry, SCHOTT has the right products in its portfolio to fulfill the highest quality demands to serve these rapidly growing market.
 
SCHOTT RealView® 2.0 lightweight

SCHOTT RealView® 2.0 lightweight

SCHOTT RealView® 2.0 lightweight sets a new benchmark for augmented reality waveguides. Featuring a novel and unique combination of outstanding optical properties, low density, and exceptional mechanical robustness, it enables lighter smart glasses with wider fields of view, excellent image quality, and the durability required for next-generation AR devices.
SCHOTT RealView® 2.0 lightweight

CHARACTERISTICS

SCHOTT RealView® 2.0 lightweight is an advanced optical glass wafer engineered for augmented reality waveguides. It combines a refractive index of 2.0 with a significantly reduced density compared to conventional high-index glasses, helping device manufacturers achieve thinner, lighter, and more comfortable AR wearables. High optical transmission and improved mechanical properties support superior image quality and long-term durability in demanding applications.

 

YOUR ADVANTAGES

  • High refractive index of 2.0 for enabling larger field of view (FoV) designs. 
  • Reduced density for lighter waveguides and improved all-day wearing comfort. 
  • Excellent optical transmission for bright, immersive AR experiences. 
  • Advanced optical glass composition combining lightweight design with strong mechanical performance. 
  • Enhanced hardness and fracture toughness for improved durability and handling robustness. 
  • Proven suitability for precision wafer manufacturing and industrial-scale production. 
  • Available in large-format wafers to support next-generation AR manufacturing platforms. 
  • Built on SCHOTT's proven AR production track record with more than 500,000 wafers shipped worldwide.
SCHOTT RealView® ultra

SCHOTT RealView® ultra

This new grade of ultra-flat wafer minimizes the fluctuation of image quality for diffractive waveguides and enables thinner and lighter devices to maintain stunning image quality.
SCHOTT RealView® ultra

CHARACTERISTICS

Decreasing glass density or wafer thickness can offer essential weight reduction for waveguides, but it comes at a price in terms of lower image quality. SCHOTT RealView® ultra not only improves wafer flatness by up to 60% but also boosts image quality, enabling AR device makers to minimize image variation between individual eye pieces and maximize production yields.

Applicable to the whole SCHOTT RealView® portfolio, this new ultra grade can also remove up to 30% of weight from the scale, and combined with the low-density SCHOTT RealView® 1.9 lightweight, SCHOTT RealView® ultra can even deliver a waveguide weight reduction of up to 50%.

 

YOUR ADVANTAGES

  • Tight flatness control minimizes light beam deflections in the waveguides to enable the highest image quality.
  • Higher tolerances for stacking multi-layer waveguides help increase manufacturing yield.
  • Thinner lightweight waveguides can be produced without compromising image quality.
  • Full immersive experience with the highest wearing comfort.
SCHOTT RealView® with titanium dioxide coatings

SCHOTT RealView® with titanium dioxide coatings

These high-refractive index wafers enable high-performance waveguides with nanostructures created by reactive ion etching.
SCHOTT RealView® with titanium dioxide coatings

CHARACTERISTICS

With a broad variety of refractive indices, SCHOTT RealView® is the leading substrate for the additive method, with index-matching resins and a subtractive approach with direct etching into the glass.

To complement SCHOTT’s portfolio for the surface relief gratings industry, SCHOTT RealView® substrates are also available with dedicated coatings for reactive ion etching (RIE) applications. In combination with high-index RealView® substrates, this opens the door for the development of highly immersive devices with large Fields of View. By using a single high-performance waveguide layer, miniaturization and weight reduction can be taken to the next level.

 

YOUR ADVANTAGES

  • Tight thickness control of TiO2 layer (nanometer range).
  • High homogeneity in pinhole-free TiO2 layer.
  • 'SCHOTT RealView® ultra' quality as the foundation for great performance.
  • Tight roughness control.
  • Strong adhesion between coating and wafer.

Want to know more? Let’s talk

Whether you need more information, samples, a quote, or advice for a project, we would be delighted to talk to you.

Contact us
Man in glasses in business office on phone while working on laptop_605x350.jpg