SCHOTT® low-loss glass is designed for advanced packaging applications. Its low dielectric constant supports broadband antenna solutions and high-frequency signal transmission. Combined with an extremely smooth surface and precise thickness control, it contributes to reliable performance in demanding communication applications.

A broadband antenna embedded in circular SCHOTT® low-loss glass

Low dielectric constant for peak performance

With its low dielectric constant of Dk = 4.0, SCHOTT® low-loss enables minimal signal delay and excellent signal transmission performance, making it ideal for broadband antenna solutions. It is particularly suited for high-frequency communication applications where reliable signal propagation is required.
Close up view of a broadband antenna

Unmatched efficiency with low dielectric loss

Featuring a low dielectric loss factor, SCHOTT® low-loss glass supports signal transmission in high-frequency applications. Its material properties help reduce dielectric losses and thermal stress, making it suitable for antenna systems, RF components and advanced IC devices.

We are certified

SCHOTT is both ISO 9001 and 14001 certified. The production of SCHOTT® low-loss is constantly monitored at all stages and all our glass is subjected to stringent quality inspection before shipping. It also complies with EU-RoHS and EU-REACH.

Want to know more? Let’s talk

Whether you need more information, samples, a quote, or advice for a project, we would be delighted to talk to you.

Contact us
Man in glasses in business office on phone while working on laptop_605x350.jpg