Does this match your preferences? Make a selection.

Technical Details of Optical Coatings

SCHOTT is able to offer an extensive range of optical coatings thanks to the consistently high technical properties of our products. This means we can improve the optical system performance for a wide range of applications and customize the spectral performance of optical components to your exact needs.

Thin film coatings for enhanced spectral performance

Outstanding transmission

Our anti-reflective and filter coatings ensure high transmission over a wide spectral range, from UV to IR. Depending on the required bandwidths and number of laser lines, transmission can be tailored to your specific needs.

High reflectivity across the range

SCHOTT offers very high reflectivity across a wide spectral range, allowing the precise steering of light to suit your application. Our portfolio of metallic and dielectric mirror coatings provides the perfect tailored solution, especially in high power laser applications and beam steering.

Outstanding durability

Our broad portfolio of durable filters and hard coatings excel in a variety of environments to ensure long-term stable performance. This performance is achieved by utilizing modern coating technologies such as magnetron and ion beam sputtering, as well as rugged filter assemblies.

High LIDT

Our dielectric mirror and AR coatings provide outstanding durability for high-power laser applications, withstanding highest laser fluence. LIDT performance can be optimized for laser type, pulse duration and wavelength.

Anti-Reflection Coatings

Anti Reflection Coatings increase the overall transmission of optical systems by minimizing surface reflections. SCHOTT offers a broad portfolio of AR coating types tailored for a wide range of applications, including imaging, Laser, and defense and aerospace, covering the wavelength range from DUV to IR.

Coating Type Wavelength Range (nm) Reflectance AOI typical LIDT Scratch / Dig Sizes up to
V-shape AR 248 - 1650 < 0.1 % 0° - 15° - Up to 20/10 Ø 300 mm
Broadband AR 248 - 1650 < 0.5 % 0° - 15° - Up to 20/10 Ø 300 mm
Scratch Resistant Hard AR 420 - 1100 < 1.5 % 0° - 30° - 40/20 up to 20/10 Ø 300 mm
Low Defect AR 380 - 780 < 0.5 % 0° - 15° - < 10/5 60 x 60 mm²
Laser Line AR 500 - 1650 < 0,2 % 0° - 15° 30 J/cm²(1064 nm, 10 ns)
10 J/cm² (532nm, 10 ns)
20/10 up to 10/5 150 x 150 mm²
Multi Line AR 248 - 1650 < 1 % 0° - 15° 20 J/cm² (1064 nm, 10 ns) 20/10 up to 10/5 Ø 300 mm

Other AOI ranges are available upon request. Reflectance depends on the required bandwidths and number of laser lines or bands. LIDT values depend on the laser type, pulse duration and wavelength.  

Mirror Coatings

SCHOTT mirrors provide the highest reflectivity for a wide spectral range, enabling the precise steering of light. Our portfolio of metallic and dielectric mirror coatings provides the ideal tailored solution, especially in high power laser applications and beam steering.

Coating Type Wavelength Range (nm) Reflectance AOI typical LIDT Scratch / Dig Sizes up to
Broadband Dielectric Mirror 248 - 1650 > 99 % 0° - 45° - Up to 20/10 Ø 300 mm
Laser Line Dielectric Mirror 248 - 1650 > 99.95 % 0° - 45° 30 J/cm²(1064 nm, 10 ns)
10 J/cm² (532nm, 10 ns)
40/20 up to 10/5 Ø 300 mm
Multi Line Dielectric Mirror 420 - 1100 > 99.9 % 0° - 45° 20 J/cm² (1064 nm, 10 ns) 40/20 up to 10/5 Ø 300 mm
Metallic Mirrors
(protective 
& enhanced)
Al: 200 - 15,000
Ag: 450- 15,000
Au: 600- 15,000
> 85 %
> 97 %
> 96 %
0° - 60° - 40/20 Ø 300 mm

Other AOI ranges are available upon request. Reflectance depends on the required bandwidths and number of laser lines or bands. LIDT values depend on the laser type, pulse duration and wavelength.

Edge and Bandpass Filters

Dielectric edge and bandpass filters enable precise control of the light spectrum. Our broad portfolio of bandpass, shortpass and longpass filters covers a broad spectral range. By utilizing IAD and sputtering, we ensure the highest precision and durability for our filters.

Coating Type Transmission
Range (nm)
Passband Transmission FWHM CWL Tolerance Slope Edge / FWHM Tolerance Blocking Range (nm) Blocking Scratch / Dig Typical Sizes (mm)
Bandpass Filter 280 - 2500 Ø > 95 % 25 – 150 nm typical +/- 1 % < 0.5 % +/- 1 % 200 – 5000 > OD3 up to
> OD6
60/40 up to 20/10 5 x 5 up to
Ø 200
Narrow Bandpass Filters 350 - 2000 Ø > 95 % < 2% CWL +/- 0.3 % < 0.5 % < 1 nm 200 – 5000 > OD 4 up to
> OD 6
60/40 up to 20/10 5 x 5 up to
Ø 100
Extremely-Narrow Bandpass Filter 450 - 1100 Ø > 90 % < 1 % CWL +/- 0.2 % < 0.5 % < 0,5 nm 200 – 5000 > OD4 up to
>
OD 6
60/40 up to 20/10 5 x 5 up to
Ø 70
Multi-Bandpass Filter 280 - 2500 Ø > 90 % 20 – 25 nm typical +/- 0.2 % < 1 % +/- 1 % 200 – 5000 > OD4 up to
>
OD 6
60/40 up to 20/10 5 x 5 up to
Ø 150
i-line Bandpass Filter 365, 405, 463 min. > 80 % < 3 nm +/- 0.2 % < 0.5 % < 0,5 nm 220 - 450 OD 2 - 3 40/20 Ø 100 up to Ø 160
UV-Bandpass Filter 200 - 350 15 - 30 % 6 - 15 nm +/- 0.5 % < 5 % < 2 % 200 - 600 > OD 4 40/20 Ø 10 up to
Ø 25
Multi-Notch Filters 280 - 2500 Ø > 90 % 20 – 25 nm typical +/- 0.2 % < 1 % < 0,5 % 200 – 5000 > OD 4 up to > OD 6 60/40 up to 20/10 5 x 5 up to
Ø 150
Steep Edge Short- & Longpass Filters 280 - 2500 Ø > 95 % - - < 0.5 % +/- 0,2 % 200 – 5000 > OD4 up to
>
OD 6
60/40 up to 20/10 5 x 5 up to
Ø 70

Want to know more? Let's talk

Whether you need more information, samples, a quote, or advice for a project, I would be delighted to talk to you.

Contact us
Man in glasses in business office on phone while working on laptop_605x350.jpg