SCHOTT® Solar Glass 0787
Protecting solar cells in high-radiation environments
Space solar cells require protection from UV exposure and high-energy particle radiation while maintaining high light transmission for power generation. SCHOTT® Solar Glass 0787 combines high optical transmission with solarization stability for photovoltaic applications in demanding radiation environments.
SCHOTT’s unique down-draw process produces ultra-thin glass with fire-polished surfaces on both sides. It is available in ultra-thin thicknesses starting from 75 µm and can be supplied as sheets or cut-to-size substrates for customer-specific designs.
Optical performance under UV and particle radiation
Exposure to UV, proton and electron radiation can cause glass to darken and lose transmission over time. The cerium-doped composition of SCHOTT® Solar Glass 0787 is designed to limit this solarization and maintain high transmission in the visible and near-infrared.
Key advantages
One glass, two functions.
Space photovoltaic cells
In orbit, UV exposure and particle radiation can gradually reduce photovoltaic performance. SCHOTT® Solar Glass 0787 forms a protective layer above the solar cell while maintaining high transmission across the spectral range used for power generation.
Optical solar reflectors
When combined with a reflective coating, SCHOTT® Solar Glass 0787 can form a thermo-optical surface for spacecraft thermal control. The glass helps shield the underlying system from solar radiation, while the coated surface supports heat exchange through infrared emittance.
Technical details
| Geometrical properties | Solar Glass 0787 | |
|---|---|---|
| Thickness portfolio* | in µm | 150 |
| 125 | ||
| 100 | ||
| 75 | ||
* Other thicknesses on request
| Optical properties | Solar Glass 0787 | |
|---|---|---|
| Refractive index nd | 1.5080 | |
| Edge wavelength λc (τ = 46 %) at t = 100 µm | nm | 332 |
| Thermal properties | Solar Glass 0787 | |
|---|---|---|
| Transformation temperature Tg | in °C | 568 |
| CTE (coefficient of thermal expansion) α(20 °C; 300 °C) | in 10-6 · K-1 | 8.5 |
| Mechanical properties | Solar Glass 0787 | |
|---|---|---|
| Density ρ | in g/cm³ | 2.51 |
| Young's modulus E | in kN/mm² | 70.0 |
| Poisson's ratio μ | 0.216 | |
FAQs
SCHOTT® Solar Glass 0787 is an ultra-thin cover glass designed for demanding space applications. It can be used to protect photovoltaic cells from UV exposure and high-energy particle radiation while maintaining high optical transmission. It is also suitable for optical solar reflector applications for spacecraft thermal control.
Yes. SCHOTT® Solar Glass 0787 is qualified according to ECSS-E-ST-20-08C for photovoltaic assemblies and components used in space applications. The applicable product configuration and qualification documentation should be confirmed for the specific project.
SCHOTT® Solar Glass 0787 is available in standard thicknesses of 0.075, 0.100, 0.125 and 0.150 mm. Other thicknesses may be available on request, depending on the project requirements.
Exposure to UV light and high-energy particle radiation can cause transmission losses in glass over time, an effect known as solarization. The cerium-doped composition of SCHOTT® Solar Glass 0787 helps reduce radiation-induced changes in optical transmission, supporting stable performance in demanding space environments.
SCHOTT® Solar Glass 0787 can be supplied with selected coating options for space applications. Anti-reflective coatings can be used to reduce reflection losses and increase usable transmission, while reflective coating configurations can support optical solar reflector applications. Available coating systems and specifications depend on the individual application and should be discussed with SCHOTT.
Yes. In addition to glass sheets, SCHOTT® Solar Glass 0787 can be supplied as cut-to-size substrates. Available dimensions, tolerances and processing options depend on the required product configuration.
Yes. SCHOTT® Solar Glass 0787 can be used as a glass substrate for optical solar reflectors (OSRs). In combination with an appropriate reflective coating, the glass can contribute to the thermal control of spacecraft by reflecting incident solar radiation while supporting infrared heat emission.
Discuss your space photovoltaic or thermal control application
Talk to SCHOTT's specialists about the required thickness, delivery form, coating and qualification documentation for your project.