Technical Details of Flexible Light Guides
Built for optimum integration
Optical
- SCHOTT multi-component Glass Optical Fibers come in a range of apertures: 0.54, 0.65 and 0.84.
 - Fused Silica for the NIR or UV range are available upon request. There are also polarisation maintaining options available.
 - Tight telecentricity and angle alignment.
 - AR coatings for best optics contact.
 
Mechanical
Design
- Diameter range from 0.5-10 mm
 - Lengths up to 10 m available
 - Single, dual or multibranch options
 - Spot to line assemblies
 - Bending radii depending on fiber and bundle diameter
 - Vacuum feedthroughs as an option
 - Cross section transformers and splitters
 
Ferrule Materials / Housings
- German Silver and Brass
 - Stainless Steel (Medical Grade)
 - Aluminum (in particular for milled housings)
 - Anodizing options upon request
 - Polymer housings milled or injection molded
 - Standard industrial connectors: SMA, ST, FC
 - Standard medical connectors: Storz, Olympus, ACMI
 
Sheathings
- Metal-PVC
 - Stainless steel interlock
 - Stainless steel interlock, covered with silicone
 - Thin wall silicone or FEP
 - Extrusion options with PVC, TPU, FEP
 
Thermal
Termination of End Surfaces
- Standard expoxy with temperature stability up to 120°C.
 - High temperature Epoxy with 200°C.
 - Hot-fused with temperature stability up to 350°C.
 
Testing
We are striving for highest quality standards. On request, we provide a variety of application specific testings that can be conducted either with SCHOTT’s own test equipment or with certified external partners. Those testings include:
- Biocompatability according to DIN 10553-5.
 - Lifetime testing in medical reprocessing tests, including cleaning and disinfection in RDG devices, autoclaving, sterrad testing and others.
 - Flammability-test IEC 60332-1-2 possible.
 - Storage and accelerated life time tests.
 - Energy chain tests for longevity in moving arm applications.
 - Cleanness and vacuum tightness of entire parts or dedicated areas.