Xensation® glass is available in a range of three distinct products: Xensation® Flex delivers revolutionary folding possibilities, Xensation® Up. offers unrivalled resistance to drop impacts, and Xensation® 3D boasts a combination of aesthetics and robust reliability. 
Xensation® Flex
Xensation® Flex

SCHOTT’s continuing research into new possibilities for glass products has produced the revolutionary new ultra-thin glass Xensation® Flex, offering a beautifully stylish, strong and highly innovative flexible product for folding devices.

CHARACTERISTICS

Xensation® Flex is the most flexible glass on Earth that is produced in a melting process, achieving a bending radius of below 2 mm with SCHOTT’s ultra-thin glass (UTG). The chemically toughenable aluminosilicate glass is available in mass production thanks to the proprietary down-draw manufacturing process that SCHOTT has been continually developing for more than 25 years.


YOUR ADVANTAGES

  • Developed for chemical toughening.
  • Highly flexible with a very small bending radius.
  • Outstanding transparency and transmission properties.
  • Fire-polished, scratch-resistant premium surface.
Xensation® Up.
Xensation® Up.

Setting an impressive new standard for chemically-strengthened lithium aluminosilicate (LAS) cover glass, Xensation® Up. offers outstanding reliability and durability for the rugged requirements of modern-day mobile electronics use, with performance in drop tests far outstripping that of conventional aluminosilicate glass.

CHARACTERISTICS

Greater flexibility and shorter processing times during the chemical strengthening stage provides processing partners with more freedom while maintaining unrivalled mechanical resistance. This is the result of a salt bath process that increases ion exchange, leading to a more stable performance.


YOUR ADVANTAGES

  • Outstanding results in set drop performance tests to ensure maximum survival of impact.
  • Superior ion exchange capabilities ensure excellent strength and processing performance.
  • Typical compressive stress (CS) and depth of layer (DoL) values are evenly balanced to deliver outstanding mechanical reliability.
Xensation® 3D
Xensation® 3D

Aesthetics can be just as important as physics in the mobile electronics market, and Xensation® 3D offers the best of both worlds, combining beauty with strength to deliver reliable high quality glass solutions for capacitive touch technologies in smartphones, wearables and other devices.

CHARACTERISTICS

Xensation® 3D offers beauty that’s built to last, thanks to impressive scratch resistance and high tolerance to the stresses and strains of everyday life. Custom-sized glass sheets are easy to cut and implement in standard production processes.


YOUR ADVANTAGES

  • Extremely high fracture-proof toughness.
  • High scratch resistance and low breakage risk.
  • Chemical strengthening parameters adjustable for different applications.
  • High light transmission.
  • Strong chemical durability.

Want to know more? Let’s talk

Whether you need more information, samples, a quote, or advice for a project, we would be delighted to talk to you.

LabelGetInTouch
Man in glasses in business office on phone while working on laptop