Technical Details of SCHOTT 8360
Lead-free physical and chemical excellence for NTC thermistors
Viscosity thermal properties
Ideal for applications where low sealing temperatures are required, such as temperature-sensitive materials that need to be hermetically protected in NTC thermistor chips.
Viscosity thermal properties  | 
        ||
|---|---|---|
| 
             Coefficient of mean linear thermal expansion   | 
            
             9,1 · 10-6 K-1  | 
        |
| 
             Transformation temperature Tg (ISO 7884-8)  | 
            
             465 °C  | 
        |
| 
             Glass temperature at viscosity ƞ in dPa · s:  | 
            
             
            1013  (annealing point) (ISO 7884-4)  | 
            
             470°C  | 
        
Electrical properties
Ideal for applications with high DK values and low dielectric loss, SCHOTT 8360 has excellent electrical insulation properties.
| 
             Electrical properties  | 
            ||
|---|---|---|
| 
             Log of the electric volume resistivity (Ω · cm)  | 
            
             at 250°C  | 
            
             8,5  | 
        
| 
             tk 100  | 
            
             275°C  | 
        |
| 
             Dielectric constant e for 1 MHz at 25°C  | 
            
             7,3  | 
        |
| 
             Dielectric loss factor tan d for 1 MHz at 25°C  | 
            
             24 1 · 10-4  | 
        |
| 
             Refractive index nd (l = 587.6 nm)  | 
            
             1.566  | 
        |