Product Variants of Optical Coatings
High Power Laser
YOUR ADVANTAGES
- High Laser Induced Damage Threshold (LIDT).
- Low-loss anti-reflective and mirror properties.
- Broad applicable wavelength range from λ 266-1560 nm.
Anti-Scratch Hard AR
 
                            
                        CHARACTERISTICS
Our patented scratch-resistant hard AR coating can be applied to SCHOTT Sapphire glass to improve light transmission without sacrificing the robustness of the material, as well as optical and technical glasses such as BOROFOLOAT 33® & Xensation® in order to greatly enhance the robustness of these materials.
YOUR ADVANTAGES
- Applicable to a wide range of materials, including SCHOTT BOROFLOAT 33®, N-BK7®, Xensation® and Sapphire.
- High blocking up to OD > 6.
- Wide applicable wavelength range from λ 400-1600 nm.
- Available as broad band AR or wide angle AR coating.
- Low reflectivity down to < 0.5%.
- Conforms to MIL-STD 675c and MIL-STD-810 standards.
Edge and Bandpass Filters
CHARACTERISTICS
Our portfolio encompasses narrow bandpass and steep edge short- and longpass filters from the UV to the NIR ranges. Utilizing IAD and sputtering techniques, we ensure our filters have the highest precision and durability.
YOUR ADVANTAGES
- High transmission for the passband T > 95% from VIS to NIR.
- High Blocking > OD 5.
- Wide blocking range from λ 200-1200 nm.
- Tight center wavelength tolerances down to +/- 0.3%.
- Edge tolerances smaller than +/- 0.5%.
- Able to combine with filter glasses for enhanced blocking > OD 8.
UV Bandpass Filters
YOUR ADVANTAGES
- Narrow bandpass with FWHM 6-15 nm.
- Passband transmission of 15-30% within λ 200-350 nm.
- Tight center wavelength tolerances down to +/- 0.5 %.
- High blocking of typical OD > 4 within a blocking range of λ 200-600 nm.
Low defect
 
                            
                        YOUR ADVANTAGES
- AR coating with typical R < 0.5% from λ 200-700 nm.
- UV-cut coating with edge position < 430 nm and tolerance +/- 6 nm.
- High environmental durability with BG-Filter glasses such as BG55.
Laser Blocking Filters
YOUR ADVANTAGES
- High transmission for the passband T > 95% from λ 400-560 nm.
- High blocking up to OD > 6.
- A wide blocking range, from λ 200 nm up to 5 µm.
- Tight center wavelength and edge tolerances.
- Able to combine with filter glasses for enhanced blocking > OD 8.
- Able to combine with Anti-Scratch Hard AR coatings for improved durability.
HMD / HUD Combiner
 
                            
                        YOUR ADVANTAGES
- High photopic transmission greater than 80%.
- High contrast over the entire projection area.
- Lowest color distortion of the outside for enhanced perception.
 
                            
                         
                            
                         
                                 
                                 
                            
                         
                            
                         
                            
                         
                                 
                                 
                                 
                            
                         
                            
                         
                                