D 263®

With high homogeneity, optical transmittance, and chemical resistance, as well as tight tolerances, D 263® has a formidable array of technical assets. Add low autofluorescence, a fire-polished surface, and a wide range of thicknesses, and you have a supremely versatile high-performance glass.

Outstanding and adaptable technical advantages

Wide range of thicknesses

While D 263® is available in a wide variety of thicknesses (from 0.03 mm to 1.1 mm, with the possibility of customized thicknesses on request), the geometrical tolerances of the glass remain consistently tight, with guaranteed quality for sheet, cut-to-size substrates and wafer.

High homogeneity

During the unique down-draw production process, SCHOTT closely monitors the optical properties of D 263®, resulting in highly homogenous sheets of glass with a refractive index accuracy of ± 0.0015. With an Abbe value of 55, it also meets the ISO 8255-1 standard for microscope cover glass.

Strong transmittance

The unique composition of D 263® and its top-quality blend of raw materials enables a high level of high optical transmittance in the UV to NIR range. A colorless appearance also helps to deliver optimum image quality, without unwanted colorization effects regardless of application.

Durable and reliable

SCHOTT D 263® performs consistently well in demanding conditions. Its high chemical resistance makes it particularly resilient in the consumer electronics, semiconductor and biotech fields.

Material Properties of D 263® M

Optical properties

Chart showing the optical properties of D 263® M

 

Thermal properties

Chart showing the thermal properties of D 263® M

 

Mechanical properties

Chart showing the mechanical properties of D 263® M

 

Spectral transmittance: 250 - 3150 nm

Chart showing the spectral transmittance (250 - 3150 nm) of D 263® M

 


Spectral transmittance: 250 - 450 nm

Chart showing the spectral transmittance (250 - 450 nm) of D 263® M

 

Transmittance values

Chart showing the transmittance values of D 263® M

 

Electrical properties

Chart showing the electrical properties of D 263® M

 

Chemical properties

Chart showing the chemical properties of D 263® M

Material properties of D 263® bio

Optical properties

Chart showing the optical properties of D 263® bio

 

Thermal properties

Chart showing the thermal properties of D 263® bio

 

Mechanical properties

Chart showing the mechanical properties of D 263® bio

 

Spectral transmittance: 250 - 3150 nm

Chart showing the spectral transmittance (250 - 3150 nm) of D 263® bio

 

Spectral transmittance: 250 - 450 nm

Chart showing the spectral transmittance (250 - 450 nm) of D 263® bio

 

Transmittance values

Chart showing the transmittance values of D 263® bio

 

Electrical properties

Chart showing the electrical properties of D 263® bio

 

Chemical properties

Chart showing the chemical properties of D 263® bio

 

Auto fluorescence in >80% transmission spectrum

Chart showing the auto fluorescence (in >80% transmission spectrum) of D 263® bio

D 263® products

SCHOTT D 263® is available as:

  • Sheets
  • Cut-to-size substrates
  • Unpolished substrates and wafers
  • FLEXINITY® 

To find out more, please see the related products on the overview page.

Want to know more? Let’s talk

Whether you need more information, samples, a quote, or advice for a project, we would be delighted to talk to you.

Get in touch
Man in glasses in business office on phone while working on laptop_605x350.jpg