PYRAN®
PYRAN® S
This monolithic, thermally tempered borosilicate glass offers exceptional quality of fire-resistant glazing and highly appealing versatility. Thanks to its outstanding optical and mechanical qualities, PYRAN® S can be found performing consistently and reliably in a broad range of landmark buildings across the world, in a wide variety of glazing designs.
CHARACTERISTICS
PYRAN® S can be designed to meet fire-resistance classes E 30 to E 120 and EW 30 to EW 60, while other key assets include clear visibility due to low residual reflection and up to two hours of additional fire protection. A butt-joint system means it can also be used within demanding architectural designs. A special silicone joint is used to join the panes of glass together without a frame. This helps to create light, smooth sheets of glass that are virtually endless, providing a clear view at all times with no disturbing vertical profiles.
YOUR ADVANTAGES
- High transmission in the visible and ultraviolet spectral ranges.
- Brilliant white glass optics, ensuring natural, pure color reproduction.
- Resistant to attack by aggressive environmental factors.
- Suitable for outdoor use with no limitations regarding UV radiation or temperature fluctuation.
- Resistant to abrasive chemical solutions.
- Option to make PYRAN® S anti-reflective on both sides using a dip-coating manufacturing process.
- Easy to use in demanding architectural designs and available in large, smooth sheets of glass for unobstructed views.
- Can also be used as part of a composite with soda-lime or single-pane safety glass, adding extra noise insulation and TRAV-certified impact resistance.
ISO PYRAN® S
ISO PYRAN® S incorporates PYRAN® S fire-resistant glass in a double-glazed unit. This offers a useful option where enhanced properties are required, not only for protection against fire but also heat and noise insulation, optimizing energy efficiency while retaining the enduring aesthetic appeal of PYRAN®.
CHARACTERISTICS
The stability of ISO PYRAN® S on exposure to UV radiation, as well as fluctuations in temperature and direct sunlight, makes it ideally suited for use in facades and roofs. While light transmission remains high, anti-glare protection is enhanced and unwanted heat and sound factors are tightly controlled.
YOUR ADVANTAGES
- Excellent sound insulation ideal for buildings in busy urban areas.
- Outstanding heat insulation and sun protection for energy efficiency.
- Excellent fire resistance qualities, with strong aesthetic appeal.
- Dip-coated anti-reflective glazing option available.
- Lamination option provides safety against falling.
PYRAN® G
While the whole PYRAN® family of products deliver outstanding fire protection, PYRAN® G offers a distinctive stunning look for many modern buildings. This curved glazing facilitates an uninterrupted, complete visual look that’s eye-catching, as well as safe and energy-efficient.
CHARACTERISTICS
PYRAN® G is a monolithic, thermally annealed borosilicate glass that takes on a distinctive cylindrical shape during the forming process. This offers a striking stylish design that increases the options for innovative architecture.
YOUR ADVANTAGES
- Excellent transparency.
- Unique look and attention-grabbing visual effect.
- Meets the requirements of fire resistance class E 30.
- While not a regulated building material, it can be used with individual building approval.
PYRAN® white
SCHOTT understands that customers not only need to meet strict fire regulations but also keep an eye on costs. PYRAN® white ticks both those boxes, meeting the requirements of fire resistance class E 30, as well as being available at very attractive prices in two different thicknesses.
CHARACTERISTICS
PYRAN® white is a monolithic, thermally annealed glass manufactured from borosilicate glass in accordance with DIN EN1748-1. Although its bending strength of 70 N/mm² is similar to soda-lime glass, it has a greater resistance to temperature change.
YOUR ADVANTAGES
- Excellent light transmission of 92 % that far exceeds that of traditional soda-lime glass.
- Attractive price and stylish appearance, with excellent safety characteristics.
- Can form a composite safety glass made of PYRAN® white and soda-lime glass to meet special noise insulation and impact protection requirements such as protection against falls.
PYRAN® Star
PYRAN® Star is a transparent fire-rated glass-ceramic for architectural application produced using SCHOTT’s rolling process.
CHARACTERISTICS
PYRAN® Star fire-rated glass-ceramics are certified by Underwriters Laboratories for fire-protection ratings. For safety-rated applications, filmed (PYRAN® Star F) and laminated (PYRAN® Star L) versions are available.
YOUR ADVANTAGES
- Transparent and wireless.
- Withstands thermal shock (hose-stream tested).
- Approximate visible light transmission of 87 %.
- Fire-rated up to 90 minutes (180 minutes in doors).
- Standard surface finish with a slight texture.
- Maximum sheet sizes: approximately 1,954 x 1,100 mm.
- Suited for use in standard fire-rated frames with the same rating.
- Conforms to positive pressure test standards.
PYRAN® Platinum
PYRAN® Platinum is the world’s first and only floated glass-ceramic developed specifically for the fire-rated glazing market, with the largest UL-tested sheet size in the industry. The new 51 x 99-inch PYRAN® Platinum sheet size lets you realize projects that were previously impossible.
CHARACTERISTICS
Architects appreciate PYRAN® Platinum's smooth surface and distortion-free finish, as well as its neutral color without amber tints and proven technical performance. PYRAN® Platinum fire-rated glass-ceramics are certified by Underwriters Laboratories. For multiple-impact applications, filmed (PYRAN® Platinum F) and laminated (PYRAN® Platinum L) versions are available.
YOUR ADVANTAGES
- Largest sheet size for a fire-rated glass-ceramic.
- Fire-rated up to 90 minutes (180 minutes in doors) and resistant to thermal shock.
- Environmentally friendly.
- Approved for use in any standard frame with the same fire rating.