SCHOTT® low-loss
Three electronic antennas embedded in SCHOTT® low-loss glass

SCHOTT® low-loss

Setting new standards for high-frequency applications, SCHOTT® low-loss glass is ready for further development as an advanced packaging material. Its low dielectric constant enables efficient broadband antenna solutions, tailored telecommunication, and precise radar applications. With an extremely smooth surface having nanometer-level precision, it ensures unrivaled performance and efficiency at GHz frequencies, paving the way for the next generation of data transmission.

A broadband antenna embedded in circular SCHOTT® low-loss glass

Low dielectric constant for peak performance

With its low dielectric constant of Dk = 4.0, SCHOTT® low-loss guarantees a minimal signal delay and highest energy efficiency, making it ideal for broadband antenna solutions. Performing on par with the best organic high frequency substrates, this material is a perfect fit for 5G/6G communication, high-speed digital circuits, and radiofrequency or microwave systems.
Close up view of a broadband antenna

Unmatched efficiency with low dielectric loss

Featuring an exceptionally low dielectric loss of tan = 0.0021@10GHz, the low-loss glass enhances radio frequency (RF) antenna and component performance. This translates to improved signal transmission, higher energy efficiency and reduced thermal stress, crucial for critical applications in space, high-frequency radars, modern telecommunication systems (5G & 6G), and advanced IoT devices.

We are certified

SCHOTT is both ISO 9001 and 14001 certified. The production of SCHOTT® low-loss is constantly monitored at all stages and all our glass is subjected to stringent quality inspection before shipping. It also complies with EU-RoHS and EU-REACH.

Want to know more? Let’s talk

Whether you need more information, samples, a quote, or advice for a project, we would be delighted to talk to you.

Contact us
Man in glasses in business office on phone while working on laptop_605x350.jpg