AR-GLAS® is acid-resistant with added versatility
AR-GLAS® is a clear soda-lime glass with acid-resistance Class S1, which makes it a reliable choice for laboratory equipment such as pipettes, as well as packaging for pharmaceuticals, cosmetics and food. It also has a high thermal expansion coefficient, making it ideal for compression seals and fusing with platinum or dumet wire.