Technical Details of VivoTag®
All the right elements for effective chip protection
Technology
The fabrication of glass tubes is one of SCHOTT's key competencies.
All high-precision cutting and sealing equipment has been developed in-house. SCHOTT VivoTag® transponder glass vials have one sealed and one fire-polished end. The fire-polishing of the open end prevents chipping during transportation and eliminates the need for further processing by protecting the electrical unit from damage during insertion into the glass vial.
Specifications
Please refer to the following table for properties of SCHOTT´s 8625 glass:
| Properties of transponder glasses | VivoTag® 8625 | 
|---|---|
| Coefficient of thermal expansion (ISO 7991) α20-300 10-6K-1 | 9.15 | 
| Transformation temperature (ISO 7884-8) °C | 514 | 
| Temperature at viscosity (ISO 884-5)104 dPas °C | 1023 | 
| Density g/cm3 | 2.52 | 
| Young's Modulus of elasticity GPa | 73 | 
| Transmission of 0.5 mm glass at 1.1 µm % | 15 | 
| 
             Classes of chemical stability water (ISO 719) acid (DIN 12116) alkali (ISO 695)  | 
            
             
 3 1 2  | 
        
| Biocompatibility | excellent, tested in animal applications | 
Dimensions
Overview of available dimensions for SCHOTT VivoTag® Tranpsonder Glass Tubes 8625*:
| AD | ID | WD | length | 
|---|---|---|---|
| 1,20 +/- 0,05 mm | 0,89 +/- 0,05 mm | +/- 0,30 mm | |
| 1,25 +/- 0,07 mm | 0,97 +/- 0,05 mm  | 
            +/- 0,30 mm | |
| 1,38 +/- 0,05 mm | 1,12 +/- 0,05 mm | +/- 0,30 mm | |
| 1,41 +/- 0,04 mm | 0,185 +/- 0,03 mm | +/- 0,30 mm | |
| 1,5 +/- 0,03 mm | 1,18 +/- 0,03 mm | +/- 0,30 mm | |
| 1,82 +/- 0,05 mm | 0,16 +/- 0,03 mm | +/- 0,30 mm | |
| 2,05 +/- 0,07 mm | 1,74 +/- 0,07 mm | +/- 0,30 mm | |
| 2,12 +/- 0,03 mm | 1,75 +/- 0,03 mm | +/- 0,30 mm | |
| 2,20 +/- 0,07 mm | 1,90 +/- 0,07 mm  | 
            +/- 0,30 mm | |
| 3,05 +/- 0,08 mm | 2,49 +/- 0,08 mm | +/- 0,30 mm | |
| 3,07 +/- 0,05 mm | 2,13 +/- 0,05 mm | +/- 0,30 mm | |
| 3,85 +/- 0,05 mm | 0,33 +/- 0,03 mm | +/- 0,30 mm | |
| 4,00 +/- 0,05 mm | 3,16 +/- 0,05 mm | +/- 0,30 mm | |
| 5,8 +/- 0,13 mm | 4,6 +/- 0,07 mm | +/- 0,30 mm  | 
        
*Subject to change – other sizes available upon request.